USA/GLOBAL: +1-949-461-9292
EUROPE: +39-011-3052-794
CONTACT US

Thermomechanical Analysis of Solder Using Nanoindentation

Solder joints are subjected to thermal and/or external stress when the temperature exceeds 0.6 Tm where Tm is the melting point of the material in Kelvin. The creep behavior of solders at elevated temperatures can directly influence the reliability of solder interconnections.  As a result, a reliable and quantitative thermomechanical analysis of the solder at different temperatures is in need. The Nano module of the Nanovea Mechanical Tester applies the load by a high-precision piezo and directly measures the evolution of force and displacement. The advanced heating oven provides a uniform temperature at the tip and sample surface, which ensures measuring accuracy and minimizes the influence of thermal drift.

Thermomechanical Analysis of Solder Using Nanoindentation

 

High Temperature Tribology

High Temperature Scratch Hardness Using Tribometer

Materials are selected based on the service requirements. For applications involving significant temperature changes and thermal gradients, it is critical to investigate the mechanical properties of materials at high temperatures to be fully aware of the mechanical limits. Materials, especially polymers, usually soften at high temperatures. A lot of mechanical failures are caused by creep deformation and thermal fatigue taking place only at elevated temperatures. Therefore, a reliable technique for measuring high temperature scratch hardness is in need to ensure proper selection of the materials for high temperature applications.

High Temperature Scratch Hardness Using Tribometer

 

In-Situ-Morphology

In Situ Morphology at High Temperature Using 3D Profilometry

High temperature environment can change the surface texture, roughness and shapes of materials, resulting in device malfunction and mechanical failures. To ensure the quality of materials or devices used at elevated temperatures, accurate and reliable in situ morphology monitoring of the shape evolution at high temperatures is in need to provide insight into the mechanism of material deformation. Moreover, real-time monitoring of surface morphology at high temperatures is very useful in materials processing, such as laser machining. The Nanovea 3D Non-Contact Profilometers measure the surface morphology of materials without touching the sample, avoiding introducing additional scratches or shape alteration which may be caused by contact technologies such as sliding stylus. Its capacity of non-contact measurement also makes it possible to measure the shape of melted samples.

In Situ Morphology at High Temperature

Portable Profilometer

Jr25 Portable Profilometer Gets New Design!

The Jr25 is the first truly portable high performance Profilometer of its kind. With an optional battery pack and carrying case, the Jr25 provides measurement capability during field studies. To enhance user convenience and control the entire portable profilometer frame has been extended as gripping handles.

Metallurgy Nanoindentation

Metallurgy Study of Multiphase Material Using Nanoindentation

Metallurgy studies the physical and chemical behavior of metallic elements, as well as their intermetallic compounds and alloys. Metals undergoing working processes, such as casting, forging, rolling, extrusion and machining, etc., change their phases, microstructure and texture, which results in varied physical properties including hardness, strength, toughness, ductility, and wear resistance. Metallography is often applied to learn the formation mechanism of such specific phases, microstructure and texture.

Metallurgy Study of Multiphase Material Using Nanoindentation

Here are examples of materials we tested this month:

mechanical-lab
Mechanical:

• Nanoindentation of multiphase metal
• Nanoindentation compression on biofilms
• Nano scratch testing of thin teflon films
• Macro scratch testing of tool coatings

profilometry-lab
3D Non-Contact Profilometry:

• Roughness of intraocular lenses
• Roughness of valve components
• Roughness of wiper blades
• Volume loss of worn dental
• Step height consistency of micro part channels

tribology-lab
Tribology:

• Wear resistance of carbon coating in lubrication

Texture Luster

Anodized Aluminum Surface Texture Effect On Luster

Anodizing is an electrolytic passivation process commonly applied to convert aluminum to aluminum oxide. It can modify the surface texture and changes the microstructure of the metal near the surface. Such an anodized aluminum oxide layer is generally much stronger and more adherent than most types of paint and metal plating. It can significantly enhance corrosion and wear resistance and improve cosmetic effects of the products. Anodized aluminum is widely used on electronic devices and consumer products, such as cell phones, cameras, mp3 players and many others.

Anodized Aluminum Surface Texture Effect On Luster

Here are examples of materials we tested this month:

mechanical-lab
Mechanical:

• Nanoindentation & scratch of thin teflon films
• Nanoindentation & Macro scratch of DLC coatings
• Microindentation ultimate tensile strength on various nickel alloys
• Micro scratch test of bio coatings

profilometry-lab
3D Non-Contact Profilometry:

• Roughness of precision machined components
• Texture of textile samples
• Coplanarity of ball grid arrays
• Volume loss of dental samples
• Flatness measurement of micro seals

tribology-lab
Tribology:

• Wear resistance of hard polymers
• Wear resistance of firearm parts
• High temperature fretting of engine parts
• Stribeck Curve of lubricants

Gold Coating Adhesion Properties

Gold Coating Adhesion on Quartz Crystal Substrate

As an extremely accurate device, the Quartz Crystal Microbalance (QCM) measures the mass change down to 0.1 nanogram. Any mass loss or delamination of the electrodes on the quartz plate will be detected by the quartz crystal and cause significant measurement errors. As a result, the intrinsic quality of the electrode gold coating and the interfacial integrity of the coating/substrate system play an essential role in performing accurate and repeatable mass measurement. The Micro scratch test is a widely used comparative measurement to evaluate the relative cohesion or adhesion properties of coatings based on comparison of the critical loads at which failures appear. It is a superior tool for reliable quality control of QCMs.

Gold Coating Adhesion on Quartz Crystal Substrate

QCM Surface Finish

Surface Finish of Quartz Crystal Microbalance

Reliable quality control heavily relies upon accurate, quantifiable and reproducible surface inspection. Flatness & finish of the Quartz Crystal Microbalance (QCM) surface are vital to its accuracy and both measurements in 3D guarantees proper manufacture processing and control measures. Unlike a touch probe technique, the Nanovea Profilometer performs a 3D non-contact surface measurement of the sample. This eliminates the risk of creating micro scratches on the QCM surface that may cause inaccuracy or errors in the mass measurement.

Surface Finish Quartz Crystal Microbalance