Vacuum Systems

Materials Testing in Vacuum

vacuum tribometer, vacuum scratch tester, vacuum hardness tester, vacuum nanoindenter, vacuum microindenter

TYPES OF TESTING

  • Hardness Tester
  • Scratch Tester
  • Friction COF Tester
  • Tribology Wear Tester
  • Non-Contact Profilometry

TESTING CONDITIONS

starting at

10 -5 TORR

VACUUM LEVEL

CUSTOM CONFIGURATIONS

Vacuum tribometer humidity module

HUMIDITY

Vacuum tribometer inert gases module

INERT GASES

Vacuum tribometer high temperature module

HIGH TEMPERATURE

MAIN INDUSTRIES

AEROSPACE

MICROELECTRONICS

What are NANOVEA vacuum testing systems?

NANOVEA vacuum systems are custom vacuum chambers built around NANOVEA instruments for materials testing in vacuum, starting at 10-5 Torr. They run hardness, scratch, friction (coefficient of friction), tribology wear and non-contact profilometry tests for materials whose service environment is a vacuum.

Each system is configured to the application, with options for humidity, inert gases and high temperature. The main industries served are aerospace and microelectronics.

Best for

  • Aerospace materials and lubricants for vacuum service
  • Microelectronics materials tested free of air and moisture

Vacuum Systems at a glance

Vacuum level
Starting at 10⁻⁵ Torr
Test types
Hardness, scratch, friction, wear, profilometry
Custom conditions
Humidity, inert gases, high temperature
Main industries
Aerospace, microelectronics

What the Vacuum Systems measures

Independent published research

NANOVEA instruments appear in 555 published studies on friction and wear, by researchers at universities and industrial laboratories worldwide.

All 555 studies →

Vacuum Systems: frequently asked questions

Why test materials in vacuum?

Friction, wear and some mechanical properties change when air and moisture are removed. Materials and coatings for aerospace and vacuum equipment are best tested in the conditions they will see in service.

What vacuum level do NANOVEA systems reach?

Starting at 10-5 Torr.

Which tests can run in a NANOVEA vacuum system?

Hardness, scratch, friction (COF), tribology wear and non-contact profilometry, with optional humidity, inert gas and high temperature control.

Are vacuum systems standard products?

No. Each is a custom configuration built around the test and the sample. Describe your application to start a design.