Why test below zero
Tires, seals, wiper blades, aircraft components, cold-chain equipment and outdoor machinery all run at sub-zero temperatures. Their materials are usually characterised at room temperature, yet cold changes tribological behaviour substantially. Elastomers stiffen and lose grip; polymers become more brittle; greases and oils thicken; moisture can freeze at the interface. Low temperature tribology measures friction and wear at the temperature the part actually sees.
How the module works
The contact is fully enclosed in a removable chamber. Cold dry air is introduced under positive pressure, which keeps the temperature uniform and stable around the sample and counterbody for the whole test. The enclosure reaches -40 °C. For colder conditions, a cryogenic adapter extends rotational and linear tests down to -150 °C.
Because the chamber surrounds the contact rather than only chilling the stage, the counterbody is at temperature as well as the sample. That matters when the counterbody’s own stiffness or surface film affects the result.
Rubber, speed and temperature
Rubber friction comes mainly from two mechanisms: adhesion at the interface, and energy lost as the rubber deforms over surface asperities. Both depend on how fast the rubber is deformed relative to its viscoelastic response, and that response shifts strongly with temperature. Cooling a rubber has an effect similar to sliding it faster, so friction measured at one temperature cannot simply be transferred to another.
NANOVEA has studied both sides of this: rubber tribology at low temperature, and rubber’s speed-dependent friction at room temperature, where COF against stainless steel rose from 0.29 to 0.8 as speed increased from 0.01 to 5 rpm. For cold-climate applications, testing across both temperature and speed gives the complete picture.
Static and dynamic friction in the cold
Breakaway (static) friction is often what limits a cold mechanism: a seal that sticks, a wiper that chatters, a slide that will not start. The tribometer’s low-speed control lets static and dynamic friction be measured in the enclosure, so stick-slip and breakaway can be compared directly with room-temperature behaviour.
Measuring the wear
After the test, the wear track is measured by chromatic confocal 3D non-contact profilometry, which works on soft and dark materials such as rubber. Worn volume gives the specific wear rate K = V / (F × s) for direct comparison across temperatures.