Blog Archives
Here are examples of materials we tested this month:

Mechanical:
• Nanoindentation of individual phases within metal cross section
• Nanoindentation hardness of thin polymer sheeting
• Macro scratch testing of titanium nitride coatings
• Macro scratch testing of Xylan coating

3D Non-Contact Profilometry:
• Roughness of nonwoven fabrics
• Topography of pipe sealant
• Coplanarity measurement of ball grid arrays
• Dimensions of aspheric lenses

Tribology:
• Friction testing of bicycle grease
• High temperature wear testing of ceramic casting material
Here are examples of materials we tested this month:

Mechanical:
• Nanoindentation of thin, hard oxide coatings
• Nanoindentation & scratch of hard titanium nitride coatings
• Microindentation compression of foams
• Microscratch of thin, hard oxide coating

3D Non-Contact Profilometry:
• Roughness & grain size analysis of dental implant
• Roughness of wood flooring finishes
• Roughness of building drywall
• Coplanarity of pin grid array under elevated temperature

Tribology:
• Wear testing of cryogenically hardened steel
• Friction testing doggie treats
• Tribocorrosion of dlc coatings
Profilometer For Large Area Measurements

Meet the ST500 Profilometer. After years of success with the ST400 and HS1000 Nanovea introduces the ST500 providing high speed large area measurement without stitching. The ST500 has a 400 mm X-Y Axis Travel, a 50 mm Z Axis with a maximum speed up to 200 mm/s. The system can be equipped with either an optical pen or line scanner for ultra fast measurement (384,000 points per second). Unlike other technologies, each point is a direct, full depth of field during large area measurement without the need of refocusing. A video zoom camera can also be used to provide automatic function to large area measurement complete on a desktop user friendly platform. See app note for example.
Scratch Adhesion Testing of Disc Coatings
In this study, instrumented scratch testing is used to assess the failure modes of the top layers of CD and BD. This test allows users to quantitatively compare the scratch resistance of different protective coatings.
Wear Evaluation by High Load Tribometer
Here are examples of materials we tested this month:

Mechanical:
• Nanoindentation & Scratch of blank coins
• Nanoindentation of electroplated coating
• Nanoindetation dma of epoxy adhesive coating

3D Non-Contact Profilometry:
• Roughness of tablet press punch
• Step height of titanium oxide films
• Dimensions of metal chamfered edge

Tribology:
• Wear testing of enriched teflon
• Wear testing of nylon composite
Corrosion Profilometry Is Application Of The Year
With the Nace Corrosion Conference only weeks away Nanovea highlights pitting corrosion measurement as its most popular profilometry application of 2014. The Nanovea Profilometer has quickly become the choice in the corrosion community for its accurate and reliable measurement. Primary area of interest include pitting depth, volume, area and density. Learn more in this months app note below.
Hardness Distribution of Hardened Metal Using Nanoindentation
In this application, the Nanovea Mechanical Tester in nanoindentation mode is used to measure the
hardness distribution of the hardened surface on the cross section of a surface hardened metal.
Hardness Distribution of Hardened Metal Using Nanoindentation
Corrosion Surface Analysis Using 3D Profilometry
In this application the Nanovea PS50 Profilometer is used to analyze the surface morphology of the
samples after service in corrosive environment. Surface roughness, materials loss and pits on the
sample surface are measured to provide more insight in the corrosion mechanism.