What lubricated testing tells you
Most real tribological contacts are lubricated, whether by oil, grease, water, a process fluid or a body fluid. Lubricated tests answer how much the fluid reduces friction and wear, under which conditions its film breaks down, and how surfaces and fluids should be paired. The difference can be dramatic: in NANOVEA’s block-on-ring study, heavy mineral oil cut friction from ~0.8 to 0.09 and reduced wear by orders of magnitude.
Two ways to lubricate the contact
Immersion. The sample sits in a liquid cup, so the contact is fully submerged throughout the test. Cups are available for rotational and linear tests, and a heating coil brings the liquid up to 150 °C. Immersion suits lubricant ranking, wear in water or saline, implant materials in simulated body fluids, and Stribeck curves.
Drop-by-drop. A metered feed applies a constant amount of lubricant to the contact. It reproduces starved or thin-film lubrication and works at high speed, even 5000 rpm, where a bath would churn or fail to form a realistic film. NANOVEA’s piston wear study used drop-by-drop feed on the T2000’s linear reciprocating stage to simulate the piston skirt and cylinder liner contact.
Stribeck curves in one run
A Stribeck curve maps friction across the lubrication regimes as speed changes: boundary, mixed and hydrodynamic. Traditionally it is assembled from many separate constant-speed tests, each with its own run-in and set-up variation. With step-less speed control, a NANOVEA tribometer ramps speed continuously, for example exponentially from 15,000 down to 0.01 rpm. The complete curve comes from one run of about 10 minutes, on one track, under one set of conditions.
Dry versus wet
The same material can rank differently dry and wet. In NANOVEA’s sandpaper study, two products of the same grit, both sold for dry and wet use, swapped places: one abraded better dry, the other wet, and in each case the condition with higher friction gave the higher abrasion rate. Testing in the actual service condition avoids that kind of surprise.
Measuring wear after lubricated tests
Lubricated wear tracks can be shallow and smooth, which makes mass loss unreliable. After cleaning, the track is measured by chromatic confocal 3D non-contact profilometry, which resolves small worn volumes and the fine morphology of polished or mildly worn surfaces. The specific wear rate follows from K = V / (F × s).