Tooth Wear Measurement Using 3D Profilometry
In this application the Nanovea ST400 Profilometer is used to measure the surface of a tooth sample mounted in epoxy that has been put through a chewing simulator. The area measured was the resulting wear and the surrounding surface area. The
maximum width, depth, perimeter, surface area, and volume lost will be used to characterize the wear track.