Step Height Measurement of Printed Electrodes
In this application the Nanovea ST400 Profilometer is used to measure printed electrodes on a flexible ceramic sheet. The area measured was large enough that it could be extrapolated to make assumptions about a much larger surface. Height and lateral dimensions will be measured to characterize the rectangular features on these samples.
Step Height Measurement of Printed Electrodes Using 3D Profilometry