Blog Archives
Here are examples of materials we tested this month:

Mechanical:
• Nanoindentation of silicon
• Nanoindentation of rubber particles
• Microscratch of metallic epoxy coatings
• Macroscratch of DLC coatings
• Microindentation UTS of titanium

3D Non-Contact Profilometry:
• Roughness of catheters
• Texture of diamond sandpaper
• Finish consistency coatings
• Topography of corroded samples
• Coplanarity of pin grid arrays
• Flatness of laser cut surface
• Motor oil lubricant friction testing
• Wear testing of DLC coatings
• Wear testing steel (Extended high temperature)
• Wear testing of DLC coatings