Here are examples of materials we tested this month:

Mechanical:
• Nanoindentation of xylan coating
• Nanoindentation composite
• Nanoindentation mapping of wood
• Nanofriction of catheter
• Nano Scratch of silicon
• Micro Scratch of silicon nitride coating

3D Non-Contact Profilometry:
• Topography of corroded steel
• Dimension of optical lens samples
• Roughness of polymer molds
• Roughness of polymer casing
• Depth of pitted aluminum
• Step height micro features
• Friction Testing of various lubricants
• Xylan coatings wear resistance
• Wear rate (high speed) of hard plastic