Surface Boundary Measurement Using 3D Profilometry
In this application the Nanovea ST400 Profilometer is used for surface boundary measurement of Styrofoam. Boundaries were established by combining a reflected intensity file along with the topography, which are simultaneously acquired using the Profilometer. This data was then used to calculate different shape and size information of each Styrofoam “grain”.