Blog Archives
Here are examples of materials we tested this month:

Mechanical:
• Nanoindentation DMA of polymer films
• Nanoindentation compression of micro features
• Nanoindentation creep of composites
• Nano Scratch of micro wire coatings
• Micro Scratch of anodized coatings
• Macroindentation multi cycle failure of micro parts
• Macro Scratch of epoxy coatings

3D Non-Contact Profilometry:
• Roughness of anodized coatings
• Laser micro etching texture measurement
• Flatness of DNA trays
• Step Height of automotive parts
• Dimensions of wafer grid

Tribology:
• Wear Testing anodized coatings
• Wear Testing epoxy coatings
• Stribeck Curve analysis of oil samples