Blog Archives
Here are examples of materials we tested this month:

Mechanical:
• Nanoindentation DMA of soft polymer
• Cermaic fracture toughness using Nanoindentation
• Nanoscratch of micro features
• Microindentation 3 Point Bend Test on pasta
• Microscratch of spray coatings

3D Non-Contact Profilometry:
• Finish of micro parts
• Texture of composite fabrics
• Roughness of various seals
• Topography of gel surfaces
• Dimensions of micro parts

Tribology:
• 24 hour Wear of various PVD coatings