In this application the Nanovea PS50 Profilometer is used to analyze the surface morphology of the
samples after service in corrosive environment. Surface roughness, materials loss and pits on the
sample surface are measured to provide more insight in the corrosion mechanism.

Corrosion Surface AnalysisUsing 3D Profilometry