Surface Finish Inspection of Wood
In this study, the Nanovea ST500 Profilometer, equipped with a line sensor and integrated optical microscope,  is used for surface finish inspection of wood samples, namely Cherry and Walnut. We showcases the capacity of Nanovea non-contact profilometer in providing fast and precise 3D finish measurement and comprehensive in-depth analysis for comparative review.

Surface Finish Inspection of Wood Using 3D Profilometry