Material properties, such as reactivity and strength, can drastically change at higher temperatures. This makes high temperature applications, (e.g. jet engines, fabrication chamber material, and even cookware) require careful material selection. Thus, it is important to understand how materials behave in different temperature conditions. The strength of a material can be measured by using the Nanovea T2000 Tribometer. To demonstrate this, a steel sample was used to conduct Brinell hardness testing from temperatures ranging from 25°C to 925°C.

1000°C Brinell Hardness w/ T2000 Tribometer