September 8-13 | Sevilla, Spain. Held every two years since 1989, the Euromat conferences gather academics and researchers from the industry with a large scope on materials science and technology and their application. The extraordinary positive evolution of the conferences in the recent editions is indicative of the materials scientist community’s excellent health.
Learn more Euromat 2013

Corrosion Measurement Using 3D Profilometry

In this application the Nanovea ST400 Profilometer is used to measure the surface of a corrosion pitted stainless steel coupon. The area measured was selected at random, and assumed large enough in that it could be extrapolated to make assumptions
about a much larger surface. Density, area, volume, size and shape will be used here to quantify the level of corrosion.

Corrosion Measurement Using 3D Profilometry

ASTM G99 Tips Perspective Continuous Wear Contact

In this application, the Nanovea Tribometer is used to measure the wear rate of a 6mm diameter Stainless Steel and Tungsten Carbide ball tip; many other custom materials and or sizes can be used. The rotative wear test (ASTM G99) was used for a 1hour duration. Then a surface profile was measured using the PS50 Profilometer and micrograph was taken to evaluate surface wear loss between each ball tip for comparison.

ASTM G99 Tips Perspective Continuous Wear Contact

2013 TRADESHOW CALENDAR

2013 Tradeshow Calender

TMS | March 4-6 San Antonio, TX
www.tms.org
AeroDef | March 19-21 Long Beach, CA
www.aerodefevent.com
MRS Spring | April 2-3 San Francisco, CA
www.mrs.org
ICMCTF | April 30-May 1 San Diego, CA
www2.avs.org
MS&T | October 29-30 Montreal, Quebec Canada
www.matscitech.org

App Notes Brochure