Pore distribution map of the yellow climbing grip sample showing detected recessed surface features across a 5 mm by 5 mm scanned area.

Pore distribution map generated from optical profilometry data of the yellow bouldering grip sample. Detected recessed features are overlaid across the 5 mm × 5 mm scanned area to visualize pore size, distribution, and surface coverage.