EE.UU./GLOBAL: +1-949-461-9292
EUROPA: +39-011-3052-794
CONTACTO

Surface Area Measurement of Oxidation With 3D Profilometry

The 3D Non Contact Perfilómetro will be used to characterize the surface area measurement of two samples with A1SiN coatings, one with a low level of silicon the other with a high level. The A1SiN coating was deposited on H13 Steel by magnetron sputtering then submitted to an oxidation resistance test (900°C-1hour).

Surface Area Measurement of Oxidation With 3D Profilometry

Tribological Characterization of Ti-WS2 Coating

In this report we will review the tribological characterization of Ti-WS2 coating deposited by Magnetron Sputtering technique. The friction and wear tribología will be obtained with the Tribometer in reciprocating mode and an integrated optical profiler will be used to obtain wear rate.

Tribological Characterization of Ti-WS2 Coating

Estos son algunos ejemplos de materiales que hemos probado este mes:

laboratorio mecánico
Mecánica:

• Nanoindentation of microseal
• Nanoindentation compression of micro ceramic
• Nanoindentation of micro rubber features
• Nano Scratch of microfeatures
• Nano Friction microtube
• Micro Scratch of engine parts
• Microindentation of coil coatings
• Resistencia al rendimiento por microindentación de microvarillas

laboratorio de perfilometría
Perfilometría 3D sin contacto:

• Topography of rubber samples
• Profile of micro parts
• Roughness of metal samples
• Roughness of wood samples
• Coplanaridad de microcaracterísticas
• Altura de los escalones de los microcanales
• Volume loss of micro pits

laboratorio de tribología
Tribología:

• Friction testing of liquid with micro particles
• Friction testing of metal samples
• Resistencia al desgaste de los recubrimientos duros
• Wear resistance of tile samples
• Wear resistance of polished concrete