3D optical profilometry reconstruction of the yellow climbing grip surface showing pores, roughness, and surface height variation.

3D rendering of the yellow bouldering grip surface measured with the NANOVEA JR25 Optical Profiler. The scan visualizes surface roughness, pore distribution, local height variation, and grip-related topographic features used for surface roughness analysis.