nano scratch testing stent coating coefficient of friction depth progression adhesion failure

Graph showing the evolution of coefficient of friction (COF) and penetration depth during nano scratch testing of a stent coating. The data illustrates coating failure progression and the transition from coating deformation to substrate support under increasing load.