EUA/GLOBAL: +1-949-461-9292
EUROPA: +39-011-3052-794
FALE CONOSCO

stent groove cross section polymer coating thickness adhesion analysis nano scratch testing

SEM cross-section of a grooved stent showing polymer coating thickness and geometry. The coating is located at the bottom of the groove, highlighting the challenge of measuring adhesion within recessed stent structures.

Tem alguma dúvida? Os especialistas da NANOVEA estão aqui para ajudar!