nano scratch testing stent coating COF depth comparison sample 1 sample 2 adhesion performance

Graph comparing coefficient of friction (COF) and penetration depth for two stent coating samples during nano scratch testing. Sample 1 shows earlier substrate contact and higher friction response, indicating lower adhesion strength compared to Sample 2.