The contact of the wear process is totally enclosed in a removable
large oven which ensures uniform and stable temperature
surrounding the sample and the counter material.
The thermal couple is either set up to be very close to the point of contact or directly touching the back on the ball inside the ball holder to
achieve the best accuracy of the temperature reading. The unique heat sink design on the main shaft of the rotative motor makes air supply sufficient for cooling.
The load cell is self-calibrated for high temperatures to ensure accurate data.