미국/글로벌: +1-949-461-9292
EUROPE: +39-011-3052-794
문의하기

stent coating sample 1 early failure nano scratch track delamination adhesion testing

Nano scratch track of Sample 1 showing early coating failure and delamination under increasing load, indicating lower coating adhesion strength.