EE.UU./GLOBAL: +1-949-461-9292
EUROPA: +39-011-3052-794
CONTACTO

Linear Module

Linear Wear Friction Test reproduces the linear reciprocating motion found in many real-world tribology mechanisms.

¿Cómo funciona?

A at, pin or ball tip is loaded onto a test sample with a precise weight.

The test samples can be of varied shape (such as cylindrical)
as long as there is a at zone of a certain length in the direction of
movement. The length of the track can be adjusted prior to starting
the measurement.

As the test starts, the tip creates a linear wear
track (zigzag pattern also possible). Because of the integrated 16bit
external position encoder, friction can be displayed for any specific
point for each pass.

This is essential to accurately study the trend of friction across the full length of the test.

See it in action

Check out our application notes where we give a sample of how you can use this module.

Tribological properties of PTFE Cookware Coatings

Honeycomb panel wear resistance using Tribometer

Versatilidad extrema

NORMAS

  • ASTM G133 
  • ASTM G171
  • ASTM F732
  • ASTM D1894
  • ASTM G132

* Los límites de los parámetros del instrumento pueden variar.
de los especificados en la norma.

Propiedades analizadas

  • Coeficiente de fricción
  • Tasas de desgaste
  • Puntos de falla
  • Resistencia eléctrica
  • Lubrication & Corrosion Studies
  • Fricción frente a velocidad
  • Dureza al rayado
  • Friction versus Load

SENSORES

  • Profundidad
  • Emisión acústica
  • Resistencia eléctrica

Muestra inferior giratoria

  • Muestras con superficie plana para la prueba.
  • Cylindrical Samples
  • Any types of materials

Muestra superior fija

  • Bola de 3, 6, 10 y 25 mm
  • Tamaños de pelotas personalizados
  • Pines personalizados
  • Placa plana
  • Geometrías personalizadas
  • Diamond, WC, Rubber and
    many other materials

Condiciones medioambientales

  • 900°C Heating Oven
  • Liquid Cup and Liquid Heating up to 150 °C
  • Lubricación gota a gota
  • Control de humedad
  • Cooling Chamber -40 °C
  • Corrosion Testing Cup
  • Varios gases
  • Vacío (personalizado)

¿Cómo podemos ayudarle?