Abbott-Firestone curve for the blue climbing grip sample showing cumulative areal material distribution and functional surface parameters.

Abbott-Firestone curve generated from optical profilometry data for the blue bouldering grip sample. The curve shows cumulative areal material distribution and supports calculation of functional surface parameters including Sk, Spk, and Svk.