EE.UU./GLOBAL: +1-949-461-9292
EUROPA: +39-011-3052-794
CONTACTO

He aquí algunos ejemplos de materiales que hemos probado este mes:

laboratorio mecánico
Mecánica:

• Nanoindentation hardness of epoxy coatings
• Nanoindentation hardness of silicone coatings
• Nanoscratch of silicone coatings
- Nanoscratch failure of stent coatings
• Nanowear friction of capillary tubes
• Microindentation compression of micro features
• Microindentation fracture of micro ceramics

laboratorio de perfilometría
Perfilometría 3D sin contacto:

• Roughness of mini turbines
• Roughness of films
• Texture of hard rubber samples
• Flatness of plastic molds
• Flatness of seal
• Depth & Area of micro channels
• Topography of oxidized samples
• Dimension of micro aerospace parts

laboratorio de tribología
Tribología:

• Friction testing various lubrications on steel
• Wear testing various hard coatings

Comentario