Morphology Measurement of Heated Polymer
In this application the Nanovea ST400 Profilometer is used for morphology measurement of polymer before and after being subjected to heat deformation. The deformation could be characterized in several ways; here we will show the change in surface area, relative volume increase and decrease and flatness as defined by ISO 12781