Tribological Properties of PTFE Using Tribometer
In this application, the wear process of a PTFE coating for non-stick pan is simulated using
Nanovea Tribometer in linear reciprocating mode. In addition, the Nanovea Mechanical
Tester was used to perform a micro scratch adhesion test to determine the critical load of
the coating adhesion failure.