<?xml version="1.0" encoding="UTF-8"?><rss version="2.0"
	xmlns:content="http://purl.org/rss/1.0/modules/content/"
	xmlns:wfw="http://wellformedweb.org/CommentAPI/"
	xmlns:dc="http://purl.org/dc/elements/1.1/"
	xmlns:atom="http://www.w3.org/2005/Atom"
	xmlns:sy="http://purl.org/rss/1.0/modules/syndication/"
	xmlns:slash="http://purl.org/rss/1.0/modules/slash/"
	>

<channel>
	<title>granica plastyczności Archiwum -</title>
	<atom:link href="https://nanovea.com/pl/tag/yield-strength/feed/" rel="self" type="application/rss+xml" />
	<link>https://nanovea.com/pl/tag/plastycznosc/</link>
	<description>Przyrządy metrologiczne do badań materiałowych i kontroli jakości</description>
	<lastBuildDate>Tue, 09 Jun 2015 18:01:16 +0000</lastBuildDate>
	<language>pl-PL</language>
	<sy:updateperiod>
	co godzinę	</sy:updateperiod>
	<sy:updatefrequency>
	1	</sy:updatefrequency>
	<generator>https://wordpress.org/?v=6.8.5</generator>

<image>
	<url>https://nanovea.com/wp-content/uploads/2025/02/nanovea-favicon.png</url>
	<title>granica plastyczności Archiwum -</title>
	<link>https://nanovea.com/pl/tag/plastycznosc/</link>
	<width>32</width>
	<height>32</height>
</image> 
	<item>
		<title>Breakthrough Measurement Proven on Steel &#038; Aluminum</title>
		<link>https://nanovea.com/pl/aktualizacja-przelomowego-pomiaru-sprawdzonego-na-stali-aluminium/?utm_source=rss&#038;utm_medium=rss&#038;utm_campaign=update-breakthrough-measurement-proven-on-steel-aluminum</link>
					<comments>https://nanovea.com/pl/aktualizacja-przelomowego-pomiaru-sprawdzonego-na-stali-aluminium/#respond</comments>
		
		<dc:creator><![CDATA[nanovea]]></dc:creator>
		<pubDate>Wed, 10 Sep 2014 20:49:59 +0000</pubDate>
				<category><![CDATA[Uncategorized]]></category>
		<category><![CDATA[yield strength]]></category>
		<guid ispermalink="false">http://nanovea.com/?p=583</guid>

					<description><![CDATA[<p>For the first time, Nanovea has developed a breakthrough method of reliably acquiring both yield strength (YS) and ultimate tensile strength (UTS) through the indentation technique; which has significant advantages when compared to the traditional tensile testing. Learn more in this months updated application note.</p>
<p>The post <a href="https://nanovea.com/pl/aktualizacja-przelomowego-pomiaru-sprawdzonego-na-stali-aluminium/">Breakthrough Measurement Proven on Steel &#038; Aluminum</a> appeared first on <a href="https://nanovea.com/pl">NANOVEA: Advanced Profilometers, Tribometers, Nanoindenters, and Scratch Testers for Materials Testing</a>.</p>
]]></description>
										<content:encoded><![CDATA[<p>Po raz pierwszy firma Nanovea opracowała przełomową metodę niezawodnego uzyskiwania zarówno granicy plastyczności (YS), jak i ostatecznej wytrzymałości na rozciąganie (UTS) poprzez <a title="mikroindentacja" href="https://nanovea.com/micro-indentation-tester" target="_blank">Technika wcięć</a>która ma znaczące zalety w porównaniu z tradycyjnymi testami rozciągania. Dowiedz się więcej w zaktualizowanym w tym miesiącu <a href="https://nanovea.com/wp-content/themes/wp-nanovea/Application%20Notes/yieldstrengthtesting.pdf" target="_blank">nota aplikacyjna</a>.</p><p>The post <a href="https://nanovea.com/pl/aktualizacja-przelomowego-pomiaru-sprawdzonego-na-stali-aluminium/">Breakthrough Measurement Proven on Steel &#038; Aluminum</a> appeared first on <a href="https://nanovea.com/pl">NANOVEA: Advanced Profilometers, Tribometers, Nanoindenters, and Scratch Testers for Materials Testing</a>.</p>
]]></content:encoded>
					
					<wfw:commentrss>https://nanovea.com/pl/aktualizacja-przelomowego-pomiaru-sprawdzonego-na-stali-aluminium/feed/</wfw:commentrss>
			<slash:comments>0</slash:comments>
		
		
			</item>
		<item>
		<title>Przełomowy test wytrzymałości na wciskanie przeprowadzony przez Nanovea</title>
		<link>https://nanovea.com/pl/breakthrough-indentation-yield-strength-test-by-nanovea/?utm_source=rss&#038;utm_medium=rss&#038;utm_campaign=breakthrough-indentation-yield-strength-test-by-nanovea</link>
					<comments>https://nanovea.com/pl/breakthrough-indentation-yield-strength-test-by-nanovea/#respond</comments>
		
		<dc:creator><![CDATA[nanovea]]></dc:creator>
		<pubDate>Wto, 08 lipca 2014 18:07:31 +0000</pubDate>
				<category><![CDATA[Press Release]]></category>
		<category><![CDATA[yield strength]]></category>
		<guid ispermalink="false">http://nanovea.com/?p=1285</guid>

					<description><![CDATA[<p>Irvine CA, July 14, 2011 – Nanovea today introduced its patent pending breakthrough method of reliably acquiring yield strength through indentation; ultimately replacing the traditional tensile testing machine for yield strength measurement. Traditionally yield strength has been tested by using a tensile testing machine, a large instrument requiring enormous strength to pull apart metal, plastic [&#8230;]</p>
<p>The post <a href="https://nanovea.com/pl/breakthrough-indentation-yield-strength-test-by-nanovea/">Breakthrough Indentation Yield Strength Test by Nanovea</a> appeared first on <a href="https://nanovea.com/pl">NANOVEA: Advanced Profilometers, Tribometers, Nanoindenters, and Scratch Testers for Materials Testing</a>.</p>
]]></description>
										<content:encoded><![CDATA[<p>Irvine, Kalifornia, 14 lipca 2011 r. - Firma Nanovea przedstawiła dziś zgłoszoną do opatentowania przełomową metodę wiarygodnego pomiaru granicy plastyczności poprzez wgłębianie, która ostatecznie zastąpi tradycyjną maszynę do prób rozciągania. Tradycyjnie granica plastyczności była badana za pomocą maszyny do prób rozciągania, dużego przyrządu wymagającego ogromnej siły do rozerwania metalu, plastiku i innych. Granica plastyczności (znana również jako granica plastyczności) materiału w inżynierii (lub materiałoznawstwie) to punkt naprężenia, w którym materiał zaczyna się odkształcać plastycznie. Przed osiągnięciem granicy plastyczności materiał odkształca się elastycznie, ale powraca do swojego pierwotnego kształtu po usunięciu naprężenia. Jest to kluczowa właściwość materiałów nano- i mikromateriałów stosowanych w rozwijających się branżach, takich jak biomedycyna, mikroelektronika, energetyka i wiele innych. Do tej pory najbardziej niezawodny sposób wymagał dużego wysiłku maszynowego, przygotowania próbki lub był niemożliwy do wykonania na małych próbkach i zlokalizowanych obszarach. Korzystając z testera mechanicznego Nanovea w trybie wgłębiania, przy użyciu cylindrycznej płaskiej końcówki, można łatwo uzyskać dane dotyczące granicy plastyczności. Od lat test wgłębiania jest wykorzystywany do pomiarów twardości i modułu sprężystości. Tradycyjnie istniał problem z powiązaniem właściwości makro rozciągania z tym, co zostało zmierzone podczas testu wgłębiania. Wiele badań z użyciem kulistych końcówek pozwoliło na uzyskanie krzywych naprężenie-odkształcenie, ale nigdy nie były one w stanie dostarczyć wiarygodnych danych dotyczących granicy plastyczności, które odpowiadałyby bezpośrednio danym dotyczącym rozciągania w skali makro. Zgłoszona do opatentowania metoda Nanovea, wykorzystująca cylindryczną płaską końcówkę, daje granicę plastyczności bezpośrednio porównywalną z tą mierzoną tradycyjnymi metodami. Uważa się, że obciążenie na powierzchnię, przy którym cylindryczna płaska końcówka penetruje przy zwiększonej prędkości, jest bezpośrednio związane z obciążeniem w stosunku do powierzchni, przy której materiał zaczyna płynąć w teście trybu rozciągania. Dlatego wiarygodne wyniki granicy plastyczności dla nieskończonej listy materiałów, małych i dużych, nigdy wcześniej nie były tak dostępne. "To tylko kolejny dodatek do długiej i stale rosnącej listy materiałów, które można badać za pomocą naszego testera mechanicznego" - powiedział Pierre Leroux, dyrektor generalny Nanovea. Chociaż ten konkretny test jest przełomem o ogromnym znaczeniu, jest to kolejny powód, dla którego Nanovea Mechanical Tester ma najszersze możliwości testowania spośród wszystkich systemów do testów mechanicznych.</p>
<p>Notę aplikacyjną można znaleźć na stronie: <a href="https://nanovea.com/wp-content/themes/wp-nanovea/Application%20Notes/yieldstrengthtesting.pdf">Przełomowe badanie wytrzymałości na wciskanie</a></p><p>The post <a href="https://nanovea.com/pl/breakthrough-indentation-yield-strength-test-by-nanovea/">Breakthrough Indentation Yield Strength Test by Nanovea</a> appeared first on <a href="https://nanovea.com/pl">NANOVEA: Advanced Profilometers, Tribometers, Nanoindenters, and Scratch Testers for Materials Testing</a>.</p>
]]></content:encoded>
					
					<wfw:commentrss>https://nanovea.com/pl/breakthrough-indentation-yield-strength-test-by-nanovea/feed/</wfw:commentrss>
			<slash:comments>0</slash:comments>
		
		
			</item>
	</channel>
</rss>