{"id":987,"date":"2014-01-07T14:00:29","date_gmt":"2014-01-07T14:00:29","guid":{"rendered":"http:\/\/nanovea.com\/?p=987"},"modified":"2015-06-16T21:34:38","modified_gmt":"2015-06-16T21:34:38","slug":"%e5%88%9d%e5%a7%8b%e5%a1%91%e6%80%a7%e5%8f%98%e5%bd%a2%e5%af%b9%e7%a3%a8%e6%8d%9f%e5%88%86%e6%9e%90%e7%9a%84%e4%b8%b4%e7%95%8c%e6%95%88%e5%ba%94","status":"publish","type":"post","link":"https:\/\/nanovea.com\/zh\/the-critical-effect-of-initial-plastic-deformation-to-wear-analysis\/","title":{"rendered":"\u521d\u59cb\u5851\u6027\u53d8\u5f62\u5bf9\u78e8\u635f\u7684\u5206\u6790"},"content":{"rendered":"<p>\u91d1\u5c5e\u6837\u54c1\uff08Cu 110\uff09\u548c\u805a\u5408\u7269\u6837\u54c1\uff08\u805a\u56db\u6c1f\u4e59\u70ef\uff09\u7684\u78e8\u635f\u8fc7\u7a0b\u4ee5\u53d7\u63a7\u548c\u76d1\u6d4b\u7684\u65b9\u5f0f\u4f7f\u7528Nanovea\u6a21\u62df\u3002 <a title=\"\u673a\u68b0\u6d4b\u8bd5\u5668\" href=\"https:\/\/nanovea\/mechanical-testers\">\u673a\u68b0\u6d4b\u8bd5\u4eea<\/a>.\u5728\u8fd9\u9879\u7814\u7a76\u4e2d\uff0c\u6211\u4eec\u60f3\u5c55\u793a\u7684\u662f\uff0c\u63a7\u5236\u548c\u6d4b\u91cf\u8d1f\u8f7d\u548c\u6df1\u5ea6\u662f\u7406\u60f3\u7684\u78e8\u635f\u5206\u6790\u65b9\u6cd5\u3002<\/p>\n<p><a href=\"https:\/\/www.nanovea.com\/Application%20Notes\/wear-test-plastic-deformation.pdf\">\u521d\u59cb\u5851\u6027\u53d8\u5f62\u5bf9\u78e8\u635f\u5206\u6790\u7684\u5173\u952e\u5f71\u54cd<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>The wear process of a metal sample (Cu 110) and a polymer sample (teflon) is simulated in controlled and monitored manner using the Nanovea Mechanical Tester. In this study, we would like to showcase that the controlling and measuring the load and depth is ideal for wear analysis. The Critical Effect Of Initial Plastic Deformation [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":988,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[140],"class_list":["post-987","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-plastic-deformation"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts\/987","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/comments?post=987"}],"version-history":[{"count":3,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts\/987\/revisions"}],"predecessor-version":[{"id":1710,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts\/987\/revisions\/1710"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/media\/988"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/media?parent=987"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/categories?post=987"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/tags?post=987"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}