{"id":2143,"date":"2015-11-24T15:44:44","date_gmt":"2015-11-24T15:44:44","guid":{"rendered":"http:\/\/nanovea.com\/?p=2143"},"modified":"2023-11-13T23:41:17","modified_gmt":"2023-11-13T23:41:17","slug":"%e7%83%ad%e5%8a%9b%e5%ad%a6-%e7%84%8a%e6%8e%a5%e5%88%86%e6%9e%90-%e4%bd%bf%e7%94%a8%e7%ba%b3%e7%b1%b3%e5%8e%8b%e7%97%95%e6%b3%95","status":"publish","type":"post","link":"https:\/\/nanovea.com\/zh\/thermomechanical-analysis-of-solder-using-nanoindentation\/","title":{"rendered":"\u5229\u7528\u7eb3\u7c73\u538b\u75d5\u5bf9\u710a\u6599\u8fdb\u884c\u70ed\u529b\u5b66\u5206\u6790"},"content":{"rendered":"<p>\u5f53\u6e29\u5ea6\u8d85\u8fc70.6\u65f6\uff0c\u710a\u70b9\u4f1a\u53d7\u5230\u70ed\u548c\/\u6216\u5916\u90e8\u5e94\u529b\u7684\u5f71\u54cd\u3002 <em>T<\/em><sub>m<\/sub> \u5176\u4e2d <em>T<\/em><sub>m<\/sub> \u662f\u6750\u6599\u7684\u7194\u70b9\uff0c\u5355\u4f4d\u662f\u5f00\u5c14\u6587\u3002\u710a\u6599\u5728\u9ad8\u6e29\u4e0b\u7684\u8815\u53d8\u884c\u4e3a\u4f1a\u76f4\u63a5\u5f71\u54cd\u710a\u6599\u4e92\u8fde\u7684\u53ef\u9760\u6027<a href=\"#_edn1\" name=\"_ednref1\">.\u00a0<\/a> \u56e0\u6b64\uff0c\u9700\u8981\u5bf9\u4e0d\u540c\u6e29\u5ea6\u4e0b\u7684\u710a\u6599\u8fdb\u884c\u53ef\u9760\u4e14\u5b9a\u91cf\u7684\u70ed\u673a\u68b0\u5206\u6790\u3002\u8fd9 <a href=\"https:\/\/nanovea.com\/nano-indentation-tester\/\">\u7eb3\u7c73\u6a21\u7ec4<\/a> \u7eb3\u8bfa\u7ef4\u4e9a <a href=\"https:\/\/nanovea.com\/mechanical-testers\/\">\u673a\u68b0\u6d4b\u8bd5\u4eea<\/a> \u901a\u8fc7\u9ad8\u7cbe\u5ea6\u538b\u7535\u65bd\u52a0\u8d1f\u8f7d\u5e76\u76f4\u63a5\u6d4b\u91cf\u529b\u548c\u4f4d\u79fb\u7684\u6f14\u53d8\u3002\u5148\u8fdb\u7684\u52a0\u70ed\u7089\u4f7f\u5c16\u7aef\u548c\u6837\u54c1\u8868\u9762\u6e29\u5ea6\u5747\u5300\uff0c\u786e\u4fdd\u6d4b\u91cf\u7cbe\u5ea6\u5e76\u6700\u5927\u9650\u5ea6\u5730\u51cf\u5c11\u70ed\u6f02\u79fb\u7684\u5f71\u54cd\u3002<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/thermomechanical-analysis.pdf\" target=\"_blank\" rel=\"noopener noreferrer\">\u5229\u7528\u7eb3\u7c73\u538b\u75d5\u5bf9\u710a\u6599\u8fdb\u884c\u70ed\u529b\u5b66\u5206\u6790<\/a><\/p>\n<p>&nbsp;<\/p>","protected":false},"excerpt":{"rendered":"<p>Solder joints are subjected to thermal and\/or external stress when the temperature exceeds 0.6 Tm where Tm is the melting point of the material in Kelvin. The creep behavior of solders at elevated temperatures can directly influence the reliability of solder interconnections.\u00a0 As a result, a reliable and quantitative thermomechanical analysis of the solder at [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":5813,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7,339],"tags":[61,15,228],"class_list":["post-2143","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","category-high-temperature-mechanical-testing","tag-mechanical-properties","tag-nanoindentation","tag-thermomechanical-analysis"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts\/2143","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/comments?post=2143"}],"version-history":[{"count":4,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts\/2143\/revisions"}],"predecessor-version":[{"id":23504,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts\/2143\/revisions\/23504"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/media\/5813"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/media?parent=2143"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/categories?post=2143"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/tags?post=2143"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}