{"id":1188,"date":"2012-07-05T23:14:57","date_gmt":"2012-07-05T23:14:57","guid":{"rendered":"http:\/\/nanovea.com\/?p=1188"},"modified":"2015-06-11T16:51:13","modified_gmt":"2015-06-11T16:51:13","slug":"%e8%bf%99%e6%98%af%e6%88%91%e4%bb%ac%e6%9c%ac%e6%9c%88%e6%b5%8b%e8%af%95%e7%9a%84%e6%9d%90%e6%96%99%e7%a4%ba%e4%be%8b-2012-07","status":"publish","type":"post","link":"https:\/\/nanovea.com\/zh\/here-are-examples-of-materials-we-tested-this-month-2012-07\/","title":{"rendered":"\u4ee5\u4e0b\u662f\u6211\u4eec\u8fd9\u4e2a\u6708\u6d4b\u8bd5\u7684\u6750\u6599\u7684\u4f8b\u5b50\u3002"},"content":{"rendered":"<p><img decoding=\"async\" class=\"alignnone size-full wp-image-825\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2015\/05\/mechanical-lab.jpg\" alt=\"\u673a\u68b0-\u5b9e\u9a8c\u5ba4\" width=\"168\" height=\"140\" \/><br \/>\n\u673a\u68b0\u3002<\/p>\n<p>- \u805a\u5408\u7269\u51dd\u80f6\u786c\u5ea6 <a title=\"\u7eb3\u7c73\u538b\u75d5\" href=\"https:\/\/nanovea.com\/nano-indentation-tester\" target=\"_blank\">\u7eb3\u7c73\u538b\u75d5<\/a> DMA<br \/>\n- \u8584\u819c\u7684\u7eb3\u7c73\u538b\u75d5\u5c48\u670d\u5f3a\u5ea6<br \/>\n- \u70ed\u6d82\u5c42\u7684\u7eb3\u7c73\u538b\u75d5\u5236\u56fe<br \/>\n- \u751f\u7269\u533b\u5b66\u6d82\u5c42\u7684\u7eb3\u7c73\u8010\u78e8\u6027<br \/>\n- \u590d\u5408\u6750\u6599\u7684\u5fae\u538b\u75d5\u65ad\u88c2<br \/>\n- \u786c\u8d28\u805a\u5408\u7269\u7684\u5fae\u5212\u75d5\u53d8\u5f62<\/p>\n<p><img decoding=\"async\" class=\"alignnone size-full wp-image-826\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2015\/05\/profilometry-lab.jpg\" alt=\"\u8f6e\u5ed3\u6d4b\u91cf-\u5b9e\u9a8c\u5ba4\" width=\"168\" height=\"140\" \/><br \/>\n\u4e09\u7ef4\u975e\u63a5\u89e6\u5f0f\u8f6e\u5ed3\u6d4b\u91cf\u6cd5\u3002<\/p>\n<p>- \u4e38\u5b50\u7684\u7c97\u7cd9\u5ea6<br \/>\n- \u7535\u5f71\u7684\u8d28\u5730<br \/>\n- \u5fae\u7f51\u7684\u8f6e\u5ed3\u4e00\u81f4\u6027<br \/>\n- \u5370\u5237\u7535\u8def\u7684\u9636\u68af\u9ad8\u5ea6<br \/>\n- \u55b7\u6d82\u7684\u5730\u5f62\u56fe<br \/>\n- \u52a0\u5de5\u7684\u805a\u5408\u7269\u90e8\u4ef6\u7684\u5c3a\u5bf8<\/p>\n<p><img decoding=\"async\" class=\"alignnone size-full wp-image-827\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2015\/05\/tribology-lab.jpg\" alt=\"\u6469\u64e6\u5b66\u5b9e\u9a8c\u5ba4\" width=\"168\" height=\"140\" \/><br \/>\n\u6469\u64e6\u5b66\u3002<\/p>\n<p>- \u5851\u6599\u7ba1\u7684\u6469\u64e6\u6d4b\u8bd5<br \/>\n- \u5851\u6599\u886c\u5957\u7684\u6469\u64e6\u6d4b\u8bd5<br \/>\n- \u94dd\u7845\u5408\u91d1\u7684\u6469\u64e6\u6d4b\u8bd5<br \/>\n- \u53d1\u52a8\u673a\u90e8\u4ef6\u7684\u78e8\u635f\u7387<br \/>\n- \u590d\u5408\u6750\u6599\u7684\u78e8\u635f\u7387<\/p>","protected":false},"excerpt":{"rendered":"<p>Mechanical: \u2022 Polymer Gel Hardness Nanoindentation DMA \u2022 Nanoindentation yield strength of films \u2022 Nanoindentation mapping of thermal coating \u2022 Nanowear of biomedical coatings \u2022 Microindentation fracture of composites \u2022 Micro Scratch deformation of hard polymers 3D Non-Contact Profilometry: \u2022 Roughness of pills \u2022 Texture of films \u2022 Profile consistence of micro mesh \u2022 Step [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[1],"tags":[112],"class_list":["post-1188","post","type-post","status-publish","format-standard","hentry","category-uncategorized","tag-polymer-gel"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts\/1188","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/comments?post=1188"}],"version-history":[{"count":3,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts\/1188\/revisions"}],"predecessor-version":[{"id":1643,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/posts\/1188\/revisions\/1643"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/media?parent=1188"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/categories?post=1188"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/zh\/wp-json\/wp\/v2\/tags?post=1188"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}