{"id":953,"date":"2014-04-06T13:33:59","date_gmt":"2014-04-06T13:33:59","guid":{"rendered":"http:\/\/nanovea.com\/?p=953"},"modified":"2015-06-16T20:58:17","modified_gmt":"2015-06-16T20:58:17","slug":"3d-profilometri-kullanarak-basili-elektrotlarin-adim-yukseklik-olcumu","status":"publish","type":"post","link":"https:\/\/nanovea.com\/tr\/step-height-measurement-of-printed-electrodes-using-3d-profilometry\/","title":{"rendered":"Bas\u0131l\u0131 Elektrotlar\u0131n Basamak Y\u00fcksekli\u011fi \u00d6l\u00e7\u00fcm\u00fc"},"content":{"rendered":"<p>Bu uygulamada Nanovea ST400 <a title=\"profilometre\" href=\"https:\/\/nanovea\/profilometers\">Profilometre<\/a> esnek bir seramik levha \u00fczerindeki bas\u0131l\u0131 elektrotlar\u0131 \u00f6l\u00e7mek i\u00e7in kullan\u0131l\u0131r. \u00d6l\u00e7\u00fclen alan, \u00e7ok daha geni\u015f bir y\u00fczey hakk\u0131nda varsay\u0131mlarda bulunmak i\u00e7in tahmin edilebilecek kadar b\u00fcy\u00fckt\u00fc. Bu \u00f6rnekler \u00fczerindeki dikd\u00f6rtgen \u00f6zellikleri karakterize etmek i\u00e7in y\u00fckseklik ve yanal boyutlar \u00f6l\u00e7\u00fclecektir.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/step-height-electrodes.pdf\">3D Profilometri Kullanarak Bas\u0131l\u0131 Elektrotlar\u0131n Basamak Y\u00fcksekli\u011fi \u00d6l\u00e7\u00fcm\u00fc<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In this application the Nanovea ST400 Profilometer is used to measure printed electrodes on a flexible ceramic sheet. The area measured was large enough that it could be extrapolated to make assumptions about a much larger surface. Height and lateral dimensions will be measured to characterize the rectangular features on these samples. Step Height Measurement [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":954,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[133],"class_list":["post-953","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-printed-electrodes"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/posts\/953","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/comments?post=953"}],"version-history":[{"count":3,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/posts\/953\/revisions"}],"predecessor-version":[{"id":1695,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/posts\/953\/revisions\/1695"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/media\/954"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/media?parent=953"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/categories?post=953"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/tags?post=953"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}