{"id":2947,"date":"2017-09-01T21:22:14","date_gmt":"2017-09-01T21:22:14","guid":{"rendered":"http:\/\/nanovea.com\/?p=2947"},"modified":"2022-03-10T16:09:14","modified_gmt":"2022-03-10T16:09:14","slug":"mikroindentasyon-haritalama-cami","status":"publish","type":"post","link":"https:\/\/nanovea.com\/tr\/microindentation-mapping-glass\/","title":{"rendered":"Cam \u00dczerinde Mikroindentasyon Haritalama"},"content":{"rendered":"<p>Mikroindentasyon haritalaman\u0131n y\u00fczey mekani\u011fi ile ilgili \u00e7al\u0131\u015fmalar i\u00e7in kritik bir ara\u00e7 oldu\u011fu kan\u0131tlanm\u0131\u015ft\u0131r. K\u0131r\u0131lma tipik olarak girintinin \u00e7atlaklar\u0131n\u0131n boyutunun \u00f6l\u00e7\u00fclmesiyle de\u011ferlendirilmi\u015ftir ve test s\u0131ras\u0131nda akustik emisyon kullan\u0131m\u0131 g\u00f6zden ka\u00e7an ve de\u011ferli bir ara\u00e7 olmu\u015ftur. <a href=\"https:\/\/nanovea.com\/micro-indentation-tester\/\">Mikroindentasyon<\/a> Akustik Emisyonlar\u0131n (AE) \u00f6l\u00e7\u00fcm\u00fc ile y\u00fckleme ve bo\u015faltma i\u015flemi s\u0131ras\u0131nda k\u0131r\u0131lma davran\u0131\u015f\u0131n\u0131 ve yo\u011funlu\u011funu izlemek i\u00e7in g\u00fcvenilir ve kullan\u0131c\u0131 dostu bir y\u00f6ntem sa\u011flar.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/App-Notes\/microindentationmapping.pdf\">Cam \u00dczerinde Mikroindentasyon Haritalama<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>Microindentation mapping has proven to be a critical tool for surface mechanics related studies. Fracture has typically been evaluated by measuring the dimension of the cracks of the indent, and the use of acoustic emission during testing has been an overlooked and valuable tool. Microindentation with the measurement of Acoustic Emissions (AE) provides a reliable [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":2948,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[296],"class_list":["post-2947","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-microindentation-mapping"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/posts\/2947","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/comments?post=2947"}],"version-history":[{"count":1,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/posts\/2947\/revisions"}],"predecessor-version":[{"id":2949,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/posts\/2947\/revisions\/2949"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/media\/2948"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/media?parent=2947"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/categories?post=2947"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/tr\/wp-json\/wp\/v2\/tags?post=2947"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}