{"id":7133,"date":"2019-11-01T20:26:57","date_gmt":"2019-11-01T20:26:57","guid":{"rendered":"https:\/\/nanovea.com\/?p=7133"},"modified":"2023-11-13T22:35:36","modified_gmt":"2023-11-13T22:35:36","slug":"tribologia-dos-polimeros","status":"publish","type":"post","link":"https:\/\/nanovea.com\/pt\/tribology-of-polymers\/","title":{"rendered":"Tribologia dos Pol\u00edmeros"},"content":{"rendered":"<div data-elementor-type=\"wp-post\" data-elementor-id=\"7133\" class=\"elementor elementor-7133\" data-elementor-post-type=\"post\">\n\t\t\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-2546c771 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"2546c771\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-5c8fd4c5\" data-id=\"5c8fd4c5\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-194d16bc elementor-widget elementor-widget-text-editor\" data-id=\"194d16bc\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p><span style=\"text-decoration: underline;\"><em><strong>Introdu\u00e7\u00e3o<\/strong><\/em><\/span><\/p>\n<p>Os pol\u00edmeros t\u00eam sido amplamente utilizados em uma ampla variedade de aplica\u00e7\u00f5es e se tornaram uma parte indispens\u00e1vel da vida cotidiana. Os pol\u00edmeros naturais como o \u00e2mbar, a seda e a borracha natural t\u00eam desempenhado um papel essencial na hist\u00f3ria da humanidade. O processo de fabrica\u00e7\u00e3o de pol\u00edmeros sint\u00e9ticos pode ser otimizado para alcan\u00e7ar propriedades f\u00edsicas \u00fanicas, tais como tenacidade, viscoelasticidade, autolubrifica\u00e7\u00e3o, e muitas outras.<\/p>\n<p><strong><u><i>Import\u00e2ncia do Desgaste e Atrito dos Pol\u00edmeros<\/i><\/u><\/strong><\/p>\n<p>Os pol\u00edmeros s\u00e3o comumente usados para aplica\u00e7\u00f5es tribol\u00f3gicas, tais como pneus, mancais e correias transportadoras.<br>Diferentes mecanismos de desgaste ocorrem dependendo das propriedades mec\u00e2nicas do pol\u00edmero, das condi\u00e7\u00f5es de contato e das propriedades dos detritos ou da pel\u00edcula de transfer\u00eancia formada durante o processo de desgaste. Para garantir que os pol\u00edmeros possuam resist\u00eancia suficiente ao desgaste sob as condi\u00e7\u00f5es de servi\u00e7o, \u00e9 necess\u00e1ria uma avalia\u00e7\u00e3o tribol\u00f3gica confi\u00e1vel e quantific\u00e1vel. A avalia\u00e7\u00e3o tribol\u00f3gica nos permite comparar quantitativamente os comportamentos de desgaste de diferentes pol\u00edmeros de forma controlada e monitorada para selecionar o material candidato para a aplica\u00e7\u00e3o alvo.<\/p>\n<p>O Nanovea Tribometer oferece testes de desgaste e atrito repet\u00edveis usando os modos rotativo e linear compat\u00edveis com ISO e ASTM, com m\u00f3dulos opcionais de desgaste e lubrifica\u00e7\u00e3o a alta temperatura dispon\u00edveis em um sistema pr\u00e9-integrado. Esta gama incompar\u00e1vel permite aos usu\u00e1rios simular os diferentes ambientes de trabalho dos pol\u00edmeros, incluindo tens\u00e3o concentrada, desgaste e alta temperatura, etc.<\/p>\n<p><strong><u><i>OBJETIVO DA MEDI\u00c7\u00c3O<\/i><\/u><\/strong><\/p>\n<p>Neste estudo, mostramos que o Nanovea <a href=\"https:\/\/nanovea.com\/tribometers\/\">Trib\u00f4metro<\/a> \u00e9 uma ferramenta ideal para comparar a resist\u00eancia ao atrito e ao desgaste de diferentes pol\u00edmeros de maneira bem controlada e quantitativa.<\/p>\n\n<p style=\"text-align: center;\"><a href=\"https:\/\/nanovea.com\/wp-content\/uploads\/2019\/11\/measurement-objective.png\"><img fetchpriority=\"high\" decoding=\"async\" class=\"wp-image-7135 aligncenter\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2019\/11\/measurement-objective.png\" alt=\"\" width=\"462\" height=\"270\"><\/a><\/p>\n<p><strong><u><i>PROCEDIMENTO DE TESTE<\/i><\/u><\/strong><\/p>\n<p>O coeficiente de atrito (COF) e a resist\u00eancia ao desgaste de diferentes pol\u00edmeros comuns foram avaliados pelo Trib\u00f4metro Nanovea. Uma bola de Al2O3 foi utilizada como contramaterial (pino, amostra est\u00e1tica). As marcas de desgaste nos pol\u00edmeros (amostras rotativas din\u00e2micas) foram medidas usando um <a href=\"https:\/\/nanovea.com\/profilometers\/\">perfil\u00f4metro 3D sem contato<\/a> e microsc\u00f3pio \u00f3ptico ap\u00f3s a conclus\u00e3o dos testes. Deve-se observar que, como op\u00e7\u00e3o, um sensor endosc\u00f3pico sem contato pode ser usado para medir a profundidade em que o pino penetra na amostra din\u00e2mica durante um teste de desgaste. Os par\u00e2metros de teste est\u00e3o resumidos na Tabela 1. A taxa de desgaste, K, foi avaliada usando a f\u00f3rmula K=Vl(Fxs), onde V \u00e9 o volume desgastado, F \u00e9 a carga normal e s \u00e9 a dist\u00e2ncia de deslizamento.<\/p>\n<p>Favor observar que as bolas Al2O3 foram usadas como material de contagem neste estudo. Qualquer material s\u00f3lido pode ser substitu\u00eddo para simular mais de perto o desempenho de dois esp\u00e9cimes sob condi\u00e7\u00f5es reais de aplica\u00e7\u00e3o.<\/p>\n\n<div style=\"text-align: center;\"><a href=\"https:\/\/nanovea.com\/wp-content\/uploads\/2017\/11\/testing-procedure.png\"><img decoding=\"async\" class=\"size-full wp-image-7343 aligncenter\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2017\/11\/testing-procedure.png\" alt=\"\" width=\"383\" height=\"729\"><\/a><\/div>\n<p><strong><u><i>RESULTADOS E DISCUSS\u00c3O<\/i><\/u><\/strong><\/p>\n<p>A taxa de desgaste \u00e9 um fator vital para determinar a vida \u00fatil dos materiais, enquanto o atrito desempenha um papel cr\u00edtico durante as aplica\u00e7\u00f5es tribol\u00f3gicas. A Figura 2 compara a evolu\u00e7\u00e3o do COF para diferentes pol\u00edmeros contra a bola Al2O3 durante os testes de desgaste. O COF funciona como um indicador de quando ocorrem falhas e o processo de desgaste entra em uma nova etapa. Entre os pol\u00edmeros testados, o HDPE mant\u00e9m o COF mais baixo constante de ~0,15 durante todo o teste de desgaste. O COF suave implica na forma\u00e7\u00e3o de um tribo-contacto est\u00e1vel.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/uploads\/2019\/11\/figure-2.png\"><img decoding=\"async\" class=\"alignnone size-full wp-image-7137\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2019\/11\/figure-2.png\" alt=\"\" width=\"870\" height=\"592\"><\/a><\/p>\n<p>As figuras 3 e 4 comparam os rastros de desgaste das amostras de pol\u00edmero ap\u00f3s o teste ser medido pelo microsc\u00f3pio \u00f3tico. O profil\u00f4metro 3D in situ sem contato determina com precis\u00e3o o volume de desgaste das amostras de pol\u00edmero, tornando poss\u00edvel calcular com precis\u00e3o taxas de desgaste de 0,0029, 0,0020 e 0,0032m3\/N m, respectivamente. Em compara\u00e7\u00e3o, a amostra de CPVC mostra a maior taxa de desgaste de 0,1121m3\/N m. As cicatrizes de desgaste paralelo profundo est\u00e3o presentes na pista de desgaste do CPVC.<\/p>\n<p style=\"text-align: center;\"><a href=\"https:\/\/nanovea.com\/wp-content\/uploads\/2019\/11\/samples-figure-3.png\"><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-7138 aligncenter\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2019\/11\/samples-figure-3.png\" alt=\"\" width=\"628\" height=\"759\"><\/a><a href=\"https:\/\/nanovea.com\/wp-content\/uploads\/2017\/11\/Blog-post-fig-5-7.png\"><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-7239 aligncenter\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2017\/11\/Blog-post-fig-5-7.png\" alt=\"\" width=\"371\" height=\"780\"><\/a><\/p>\n<p><strong><u><i>CONCLUS\u00c3O<\/i><\/u><\/strong><\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/uploads\/2017\/11\/tire.png\"><img loading=\"lazy\" decoding=\"async\" class=\"alignnone wp-image-7241\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2017\/11\/tire.png\" alt=\"\" width=\"897\" height=\"349\"><\/a><\/p>\n<p>A resist\u00eancia ao desgaste dos pol\u00edmeros tem um papel vital em seu desempenho de servi\u00e7o. Neste estudo, mostramos que o Nanovea Tribometer avalia o coeficiente de atrito e a taxa de desgaste de diferentes pol\u00edmeros em um<br>bem controlada e de maneira quantitativa. O PEAD apresenta o menor COF de ~0,15 entre os pol\u00edmeros testados. As amostras de PEAD, Nylon 66, e Polipropileno possuem baixas taxas de desgaste de 0,0029, 0,0020 e 0,0032 m3\/N m, respectivamente. A combina\u00e7\u00e3o de baixo atrito e grande resist\u00eancia ao desgaste faz do PEAD um bom candidato para aplica\u00e7\u00f5es tribol\u00f3gicas de pol\u00edmeros.<\/p>\n<p>O profil\u00f4metro 3D sem contato in situ permite a medi\u00e7\u00e3o precisa do volume de desgaste e oferece uma ferramenta para analisar a morfologia detalhada das faixas de desgaste, fornecendo mais informa\u00e7\u00f5es sobre a compreens\u00e3o fundamental dos mecanismos de desgaste<\/p>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-b8e4b47 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"b8e4b47\" data-element_type=\"section\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-1b34de4\" data-id=\"1b34de4\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-12614d6 elementor-widget elementor-widget-heading\" data-id=\"12614d6\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\"><b>AGORA, VAMOS FALAR SOBRE SUA APLICA\u00c7\u00c3O<\/b><\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-8bd4570 live-chat elementor-align-center elementor-widget elementor-widget-button\" data-id=\"8bd4570\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-md\" href=\"https:\/\/nanovea.com\/contact\/live-chat\/\" id=\"live-chat\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">CHAT AO VIVO<\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<\/div>","protected":false},"excerpt":{"rendered":"<p>Download PDF version Introduction Polymers have been used extensively in a wide variety of applications and have become an indispensable part of everyday life. Natural polymers such as amber, silk, and natural rubber have played an essential role in human history. The fabrication process of synthetic polymers can be optimized to achieve unique physical properties [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":11715,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7,349,355,335,373,336],"tags":[],"class_list":["post-7133","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","category-laboratory-testing","category-profilometry-volume-area","category-profilometry-testing","category-rotational-tribology","category-tribology-testing"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/posts\/7133","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/comments?post=7133"}],"version-history":[{"count":45,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/posts\/7133\/revisions"}],"predecessor-version":[{"id":23426,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/posts\/7133\/revisions\/23426"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/media\/11715"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/media?parent=7133"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/categories?post=7133"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/tags?post=7133"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}