{"id":2394,"date":"2016-05-24T14:31:58","date_gmt":"2016-05-24T14:31:58","guid":{"rendered":"http:\/\/nanovea.com\/?p=2394"},"modified":"2016-05-24T14:31:58","modified_gmt":"2016-05-24T14:31:58","slug":"3d-wear-track-scan-situ-tribometro","status":"publish","type":"post","link":"https:\/\/nanovea.com\/pt\/3d-wear-track-scan-situ-tribometer\/","title":{"rendered":"Varredura de trilha de desgaste 3D em Situ no Trib\u00f4metro"},"content":{"rendered":"<p>Convencional pin-on-disc ou rec\u00edproco <a href=\"https:\/\/nanovea.com\/tribometers\">trib\u00f4metro<\/a> registra o COF durante o teste de desgaste. A taxa de desgaste \u00e9 medida ap\u00f3s o teste de desgaste, movendo a amostra para um profil\u00f4metro e escaneando os perfis da se\u00e7\u00e3o transversal da pista de desgaste. Tal m\u00e9todo pode introduzir erros quando a amostra possui uma pista de desgaste n\u00e3o homog\u00eanea. Al\u00e9m disso, amostras como os revestimentos multicamadas possuem diferentes resist\u00eancias ao desgaste em diferentes camadas do revestimento. Uma t\u00e9cnica mais confi\u00e1vel e repet\u00edvel para avalia\u00e7\u00e3o do desgaste \u00e9 necess\u00e1ria - a Nanovea desenvolveu um trib\u00f4metro equipado com um profil\u00f4metro 3D sem contato que realiza uma varredura 3D da pista de desgaste completa no est\u00e1gio de amostra do trib\u00f4metro. Ele monitora a evolu\u00e7\u00e3o da morfologia da pista de desgaste 3D, permitindo aos usu\u00e1rios calcular com precis\u00e3o a taxa de desgaste e determinar o modo de falha em diferentes est\u00e1gios usando uma amostra de teste.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/3d-wear-track.pdf\">Varredura de trilha de desgaste 3D em Situ no Trib\u00f4metro<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>Conventional pin-on-disc or reciprocating tribometer records the COF during the wear test. The wear rate is measured after the wear test by moving the sample to a profilometer and scanning the cross section profiles of the wear track. Such a method may introduce errors when the sample possesses an inhomogeneous wear track. Moreover, samples like [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":2399,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[246],"class_list":["post-2394","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-3d-wear-track"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/posts\/2394","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/comments?post=2394"}],"version-history":[{"count":3,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/posts\/2394\/revisions"}],"predecessor-version":[{"id":2401,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/posts\/2394\/revisions\/2401"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/media\/2399"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/media?parent=2394"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/categories?post=2394"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/pt\/wp-json\/wp\/v2\/tags?post=2394"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}