{"id":961,"date":"2014-03-07T13:38:51","date_gmt":"2014-03-07T13:38:51","guid":{"rendered":"http:\/\/nanovea.com\/?p=961"},"modified":"2015-06-16T21:05:32","modified_gmt":"2015-06-16T21:05:32","slug":"elastyczna-plastyczna-reakcja-powloki-polimerowej-pod-powtarzajacym-sie-uderzeniem","status":"publish","type":"post","link":"https:\/\/nanovea.com\/pl\/elastic-plastic-response-of-polymer-coating-under-repetitive-impact\/","title":{"rendered":"Elastyczno-plastyczna reakcja pow\u0142oki polimerowej"},"content":{"rendered":"<p>W tym zastosowaniu zaprojektowali\u015bmy now\u0105 konfiguracj\u0119 testow\u0105, aby symulowa\u0107 powtarzaj\u0105ce si\u0119 uderzenia w elementy ochronne.<br \/>\ni zbadano jej reakcj\u0119 spr\u0119\u017cysto-plastyczn\u0105 w funkcji czasu przy u\u017cyciu Nanovea<br \/>\nTester mechaniczny w <a title=\"mikroindentacja\" href=\"https:\/\/nanovea\/micro-indentation-tester\" target=\"_blank\">Mikroindentacja<\/a> tryb.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/elastic-plastic-response.pdf\">Elastyczno-plastyczna reakcja pow\u0142oki polimerowej na powtarzaj\u0105ce si\u0119 uderzenia<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In this application, we designed a new testing setup to simulate the repetitive impact on the protective polymer coating and investigated its elastic-plastic response as a function of time using the Nanovea Mechanical Tester in Microindentation mode. Elastic-Plastic Response of Polymer Coating Under Repetitive Impact<\/p>","protected":false},"author":1,"featured_media":962,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[134],"class_list":["post-961","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-elastic-plastic"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/posts\/961","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/comments?post=961"}],"version-history":[{"count":4,"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/posts\/961\/revisions"}],"predecessor-version":[{"id":11384,"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/posts\/961\/revisions\/11384"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/media\/962"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/media?parent=961"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/categories?post=961"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/pl\/wp-json\/wp\/v2\/tags?post=961"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}