{"id":987,"date":"2014-01-07T14:00:29","date_gmt":"2014-01-07T14:00:29","guid":{"rendered":"http:\/\/nanovea.com\/?p=987"},"modified":"2015-06-16T21:34:38","modified_gmt":"2015-06-16T21:34:38","slug":"%ec%b4%88%ea%b8%b0-%ec%86%8c%ec%84%b1-%eb%b3%80%ed%98%95-%eb%a7%88%eb%aa%a8-%eb%b6%84%ec%84%9d%ec%9d%98-%ec%9e%84%ea%b3%84-%ed%9a%a8%ea%b3%bc","status":"publish","type":"post","link":"https:\/\/nanovea.com\/ko\/the-critical-effect-of-initial-plastic-deformation-to-wear-analysis\/","title":{"rendered":"\ub9c8\ubaa8\uc5d0 \ub530\ub978 \ucd08\uae30 \uc18c\uc131 \ubcc0\ud615 \ubd84\uc11d"},"content":{"rendered":"<p>\uae08\uc18d \uc2dc\ub8cc(Cu 110)\uc640 \ud3f4\ub9ac\uba38 \uc2dc\ub8cc(\ud14c\ud50c\ub860)\uc758 \ub9c8\ubaa8 \uacf5\uc815\uc740 \ub098\ub178\ubca0\uc544\ub97c \uc0ac\uc6a9\ud558\uc5ec \uc81c\uc5b4 \ubc0f \ubaa8\ub2c8\ud130\ub9c1 \ubc29\uc2dd\uc73c\ub85c \uc2dc\ubbac\ub808\uc774\uc158\ub429\ub2c8\ub2e4. <a title=\"\uae30\uacc4\uc2dd \ud14c\uc2a4\ud130\" href=\"https:\/\/nanovea\/mechanical-testers\">\uae30\uacc4 \ud14c\uc2a4\ud130<\/a>. \uc774 \uc5f0\uad6c\uc5d0\uc11c\ub294 \ud558\uc911\uacfc \uae4a\uc774\ub97c \uc81c\uc5b4\ud558\uace0 \uce21\uc815\ud558\ub294 \uac83\uc774 \ub9c8\ubaa8 \ubd84\uc11d\uc5d0 \uc774\uc0c1\uc801\uc774\ub77c\ub294 \uac83\uc744 \ubcf4\uc5ec\uc8fc\uace0\uc790 \ud569\ub2c8\ub2e4.<\/p>\n<p><a href=\"https:\/\/www.nanovea.com\/Application%20Notes\/wear-test-plastic-deformation.pdf\">\ucd08\uae30 \uc18c\uc131 \ubcc0\ud615\uc774 \ub9c8\ubaa8 \ubd84\uc11d\uc5d0 \ubbf8\uce58\ub294 \uc911\uc694\ud55c \uc601\ud5a5<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>The wear process of a metal sample (Cu 110) and a polymer sample (teflon) is simulated in controlled and monitored manner using the Nanovea Mechanical Tester. In this study, we would like to showcase that the controlling and measuring the load and depth is ideal for wear analysis. The Critical Effect Of Initial Plastic Deformation [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":988,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[140],"class_list":["post-987","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-plastic-deformation"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/posts\/987","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/comments?post=987"}],"version-history":[{"count":3,"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/posts\/987\/revisions"}],"predecessor-version":[{"id":1710,"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/posts\/987\/revisions\/1710"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/media\/988"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/media?parent=987"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/categories?post=987"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/ko\/wp-json\/wp\/v2\/tags?post=987"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}