{"id":3383,"date":"2018-06-04T17:26:44","date_gmt":"2018-06-04T17:26:44","guid":{"rendered":"https:\/\/nanovea.com\/?p=3383"},"modified":"2019-08-06T21:16:57","modified_gmt":"2019-08-06T21:16:57","slug":"%e3%82%b3%e3%83%b3%e3%82%af%e3%83%aa%e3%83%bc%e3%83%88%e7%b2%97%e3%81%95%e3%83%9d%e3%83%bc%e3%82%bf%e3%83%96%e3%83%ab%e3%83%97%e3%83%ad%e3%83%95%e3%82%a1%e3%82%a4%e3%83%ab%e6%b8%ac%e5%ae%9a","status":"publish","type":"post","link":"https:\/\/nanovea.com\/ja\/concrete-roughness-portable-profilometry\/","title":{"rendered":"\u643a\u5e2f\u578b3\u6b21\u5143\u5f62\u72b6\u6e2c\u5b9a\u5668\u306b\u3088\u308b\u30b3\u30f3\u30af\u30ea\u30fc\u30c8\u7c97\u3055\u306e\u6e2c\u5b9a"},"content":{"rendered":"<p>\u5f93\u6765\u306f\u3001\u8a66\u6599\u3092\u30b9\u30c6\u30fc\u30b8\u306b\u8a2d\u7f6e\u3059\u308b\u3053\u3068\u304c\u56f0\u96e3\u3067\u3042\u3063\u305f\u305f\u3081\u3001\u6e2c\u5b9a\u304c\u56f0\u96e3\u3067\u3057\u305f\u3002\u30ca\u30ce\u30d9\u30a2\u306eJR25\u3067\u306f\u3001\u8a66\u6599\u3092\u8a2d\u7f6e\u3059\u308b\u5fc5\u8981\u304c\u306a\u304f\u3001\u52d5\u304b\u3055\u306a\u3051\u308c\u3070\u3088\u3044\u306e\u3067\u3059\u3002\u305d\u306e\u305f\u3081\u3001\u58c1\u3084\u8eca\u3001\u6a5f\u68b0\u306a\u3069\u306e\u5927\u304d\u306a\u5bfe\u8c61\u7269\u3082\u5bb9\u6613\u306b\u30b9\u30ad\u30e3\u30f3\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002\u307e\u305f\u3001\u30b3\u30f3\u30d1\u30af\u30c8\u306a\u30b5\u30a4\u30ba\u306a\u306e\u3067\u3001\u6301\u3061\u904b\u3073\u304c\u3067\u304d\u3001\u591a\u69d8\u306a\u4f7f\u3044\u65b9\u304c\u3067\u304d\u307e\u3059\u3002\u307e\u305f\u3001\u30da\u30f3\u578b\u30bb\u30f3\u30b5\u30fc\u3092\u659c\u3081\u306b\u50be\u3051\u308b\u3053\u3068\u304c\u3067\u304d\u308b\u305f\u3081\u3001\u5e73\u3089\u3067\u306a\u304f\u3001\u30d7\u30ed\u30fc\u30d6\u304c\u5f53\u305f\u308a\u306b\u304f\u3044\u30b5\u30f3\u30d7\u30eb\u306e\u6e2c\u5b9a\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u30023D\u30ce\u30f3\u30b3\u30f3\u30bf\u30af\u30c8 <a href=\"https:\/\/nanovea.com\/profilometers\/\">\u30d7\u30ed\u30d5\u30a3\u30ed\u30e1\u30fc\u30bf\u30fc<\/a> \u307e\u305f\u3001\u8ef8\u8272\u6280\u8853\u3092\u7528\u3044\u308b\u3053\u3068\u3067\u3001\u6700\u5c0f\u9650\u306e\u8a66\u6599\u6e96\u5099\u3067\u3042\u3089\u3086\u308b\u8868\u9762\u306e\u6e2c\u5b9a\u304c\u53ef\u80fd\u3067\u3059\u3002\u30ca\u30ce\u304b\u3089\u30de\u30af\u30ed\u306e\u9ad8\u3055\u3092\u3001\u8a66\u6599\u306e\u53cd\u5c04\u7387\u3001\u900f\u660e\u5ea6\u3001\u66f2\u7387\u306e\u5f71\u97ff\u3092\u53d7\u3051\u305a\u306b\u6e2c\u5b9a\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002\u30ca\u30ce\u30d9\u30a2\u30fc\u306eJR25 3D\u975e\u63a5\u89e6\u30d7\u30ed\u30d5\u30a3\u30ed\u30e1\u30fc\u30bf\u30fc\u306f\u3001\u67d4\u8edf\u6027\u3068\u643a\u5e2f\u6027\u306b\u512a\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u5f93\u6765\u306e\u30d7\u30ed\u30d5\u30a3\u30ed\u30e1\u30fc\u30bf\u30fc\u3068\u6bd4\u8f03\u3057\u3066\u3001\u3088\u308a\u5e83\u7bc4\u56f2\u306e\u30b5\u30f3\u30d7\u30eb\u3092\u7c21\u5358\u306b\u6e2c\u5b9a\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002<\/p>\n<p><a href=\"http:\/\/nanovea.com\/App-Notes\/Portability-and-Flexibility-of-the-Nanovea-Jr25.pdf\">\u643a\u5e2f\u578b3\u6b21\u5143\u5f62\u72b6\u6e2c\u5b9a\u5668\u306b\u3088\u308b\u30b3\u30f3\u30af\u30ea\u30fc\u30c8\u7c97\u3055\u306e\u6e2c\u5b9a<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>Measurement of nonconventional samples is difficult mainly due to problems mounting the sample onto a stage. For Nanovea\u2019s JR25, the sample does not need to be mounted; it just has to remain unmoving. This means large objects such as walls, cars, or machines can be easily scanned. Its compact size makes it portable as well as diverse. It can tilt its pen sensor at an angle which makes it ideal in measuring samples that are not flat and have difficulties exposing its area of interest to a scanning probe. Since the 3D Non-Contact Profilometer uses axial chromatism technology, it can also measure any surface with minimal sample preparation. Nano to [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":3387,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[313,312],"class_list":["post-3383","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-concrete-roughness","tag-portble-profilometry"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/posts\/3383","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/comments?post=3383"}],"version-history":[{"count":4,"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/posts\/3383\/revisions"}],"predecessor-version":[{"id":6758,"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/posts\/3383\/revisions\/6758"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/media\/3387"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/media?parent=3383"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/categories?post=3383"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/ja\/wp-json\/wp\/v2\/tags?post=3383"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}