{"id":953,"date":"2014-04-06T13:33:59","date_gmt":"2014-04-06T13:33:59","guid":{"rendered":"http:\/\/nanovea.com\/?p=953"},"modified":"2015-06-16T20:58:17","modified_gmt":"2015-06-16T20:58:17","slug":"mesure-de-la-hauteur-des-electrodes-imprimees-utilisant-la-profilometrie-3d","status":"publish","type":"post","link":"https:\/\/nanovea.com\/fr\/step-height-measurement-of-printed-electrodes-using-3d-profilometry\/","title":{"rendered":"Mesure de la hauteur de pas des \u00e9lectrodes imprim\u00e9es"},"content":{"rendered":"<p>Dans cette application, le Nanovea ST400 <a title=\"profilom\u00e8tre\" href=\"https:\/\/nanovea\/profilometers\">Profilom\u00e8tre<\/a> est utilis\u00e9 pour mesurer des \u00e9lectrodes imprim\u00e9es sur une feuille de c\u00e9ramique flexible. La surface mesur\u00e9e \u00e9tait suffisamment grande pour pouvoir \u00eatre extrapol\u00e9e afin de faire des hypoth\u00e8ses sur une surface beaucoup plus grande. La hauteur et les dimensions lat\u00e9rales seront mesur\u00e9es pour caract\u00e9riser les caract\u00e9ristiques rectangulaires sur ces \u00e9chantillons.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/step-height-electrodes.pdf\">Mesure de la hauteur de pas des \u00e9lectrodes imprim\u00e9es \u00e0 l'aide de la profilom\u00e9trie 3D<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In this application the Nanovea ST400 Profilometer is used to measure printed electrodes on a flexible ceramic sheet. The area measured was large enough that it could be extrapolated to make assumptions about a much larger surface. Height and lateral dimensions will be measured to characterize the rectangular features on these samples. Step Height Measurement [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":954,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[133],"class_list":["post-953","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-printed-electrodes"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/953","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/comments?post=953"}],"version-history":[{"count":3,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/953\/revisions"}],"predecessor-version":[{"id":1695,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/953\/revisions\/1695"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/media\/954"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/media?parent=953"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/categories?post=953"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/tags?post=953"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}