{"id":818,"date":"2015-03-05T15:51:04","date_gmt":"2015-03-05T15:51:04","guid":{"rendered":"http:\/\/nanovea.com\/?p=818"},"modified":"2015-06-17T16:20:22","modified_gmt":"2015-06-17T16:20:22","slug":"essai-dadherence-des-revetements-de-disques-par-rayures","status":"publish","type":"post","link":"https:\/\/nanovea.com\/fr\/scratch-adhesion-testing-of-disc-coatings\/","title":{"rendered":"Test d'adh\u00e9rence des rev\u00eatements de disques aux rayures"},"content":{"rendered":"<p>Dans cette \u00e9tude, des instruments <a title=\"tests de micro-rayures\" href=\"https:\/\/nanovea.com\/micro-scratch-tester\" target=\"_blank\">test de grattage<\/a> est utilis\u00e9 pour \u00e9valuer les modes de d\u00e9faillance des couches sup\u00e9rieures de CD et BD. Ce test permet aux utilisateurs de comparer quantitativement la r\u00e9sistance aux rayures de diff\u00e9rents rev\u00eatements de protection.<\/p>\n<p><a title=\"test d&#039;adh\u00e9sion aux rayures\" href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/CompactDiscCoatings.pdf\" target=\"_blank\">Test d'adh\u00e9rence des rev\u00eatements de disques aux rayures<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In this study, instrumented scratch testing is used to assess the failure modes of the top layers of CD and BD. This test allows users to quantitatively compare the scratch resistance of different protective coatings. Scratch Adhesion Testing of Disc Coatings<\/p>","protected":false},"author":1,"featured_media":819,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[150],"class_list":["post-818","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-adhesion-testing"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/818","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/comments?post=818"}],"version-history":[{"count":7,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/818\/revisions"}],"predecessor-version":[{"id":1578,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/818\/revisions\/1578"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/media\/819"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/media?parent=818"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/categories?post=818"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/tags?post=818"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}