{"id":1957,"date":"2015-08-26T20:28:23","date_gmt":"2015-08-26T20:28:23","guid":{"rendered":"http:\/\/nanovea.com\/?p=1957"},"modified":"2015-08-26T20:38:01","modified_gmt":"2015-08-26T20:38:01","slug":"cartographie-des-proprietes-mecaniques","status":"publish","type":"post","link":"https:\/\/nanovea.com\/fr\/mechanical-property-mapping\/","title":{"rendered":"Outil de cartographie des propri\u00e9t\u00e9s m\u00e9caniques Broadview"},"content":{"rendered":"<p>Vous voyez ci-dessus un exemple de l'outil de s\u00e9lection de carte Broadview de Nanovea, en attente de brevet. Ce nouvel outil permet aux utilisateurs de s\u00e9lectionner facilement n'importe quel emplacement sur une large vue de surface cousue de l'\u00e9chantillon. En outre, l'utilisateur peut s\u00e9lectionner tous les param\u00e8tres de test \u00e0 chaque emplacement, que ce soit pour un test unique ou une cartographie multi-tests. Tous les emplacements et param\u00e8tres de test peuvent \u00eatre enregistr\u00e9s dans des recettes facilement r\u00e9cup\u00e9rables. Cette avanc\u00e9e significative permet des \u00e9tudes rapides et conviviales des propri\u00e9t\u00e9s m\u00e9caniques de la nano \u00e0 la macro. Pour en savoir plus, consultez la note d'application de ce mois-ci : <a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/mechanical-mapping.pdf\" target=\"_blank\">Cartographie des propri\u00e9t\u00e9s m\u00e9caniques<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>Seen above is an example of Nanovea&#8217;s patent pending Broadview Map Selection Tool. This new tool allows users easy selection of any location on a broad stitched surface view of the sample. Additionally, the user can select all testing parameters at each location, either for a one test or a multi-tests mapping. All locations and [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":1958,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[203],"class_list":["post-1957","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-mechanical-property-mapping"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/1957","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/comments?post=1957"}],"version-history":[{"count":2,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/1957\/revisions"}],"predecessor-version":[{"id":1964,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/1957\/revisions\/1964"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/media\/1958"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/media?parent=1957"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/categories?post=1957"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/tags?post=1957"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}