{"id":1197,"date":"2012-05-07T23:23:21","date_gmt":"2012-05-07T23:23:21","guid":{"rendered":"http:\/\/nanovea.com\/?p=1197"},"modified":"2015-06-17T21:37:20","modified_gmt":"2015-06-17T21:37:20","slug":"resistance-a-la-fracture-du-silicium-avec-test-de-nano-rayures","status":"publish","type":"post","link":"https:\/\/nanovea.com\/fr\/fracture-resistance-of-silicon-with-nano-scratch-testing\/","title":{"rendered":"R\u00e9sistance \u00e0 la rupture du silicium par des tests de nano-rayures"},"content":{"rendered":"<p>Dans cette application, le testeur m\u00e9canique Nanovea, en nano <a title=\"test de grattage\" href=\"https:\/\/nanovea.com\/nano-scratch-tester\">test de grattage<\/a> mode, est utilis\u00e9 pour mesurer la r\u00e9sistance \u00e0 la rupture d'un \u00e9chantillon de silicium de 170\u03bcm d'\u00e9paisseur. Nous devons simuler le processus de grattage de mani\u00e8re contr\u00f4l\u00e9e et surveill\u00e9e pour observer les effets du comportement de l'\u00e9chantillon.  Un stylet \u00e0 pointe de diamant de 2\u03bcm est utilis\u00e9 \u00e0 une charge progressive allant de 0,5 mN \u00e0 400 mN pour rayer la surface du silicium. Les points de d\u00e9faillance seront examin\u00e9s.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/fracture-resistance.pdf\">R\u00e9sistance \u00e0 la rupture du silicium par des tests de nano-rayures <\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In this application, the Nanovea Mechanical Tester, in nano scratch testing mode, is used to measure the fracture resistance of a 170\u03bcm thick silicon sample. We must simulate the process of scratching in a controlled and monitored manner to observe sample behavior effects.\u00a0 A 2\u03bcm diamond tipped stylus is used at a progressive load ranging [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":1198,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[173],"class_list":["post-1197","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-fracture-resistance"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/1197","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/comments?post=1197"}],"version-history":[{"count":3,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/1197\/revisions"}],"predecessor-version":[{"id":1782,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/posts\/1197\/revisions\/1782"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/media\/1198"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/media?parent=1197"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/categories?post=1197"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/fr\/wp-json\/wp\/v2\/tags?post=1197"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}