{"id":858,"date":"2014-11-09T02:34:24","date_gmt":"2014-11-09T02:34:24","guid":{"rendered":"http:\/\/nanovea.com\/?p=858"},"modified":"2015-10-07T20:03:15","modified_gmt":"2015-10-07T20:03:15","slug":"automated-multi-sample-scratch-testing","status":"publish","type":"post","link":"https:\/\/nanovea.com\/es\/automated-multi-sample-scratch-testing\/","title":{"rendered":"Prueba de rayado automatizada de m\u00faltiples muestras"},"content":{"rendered":"<p>En esta aplicaci\u00f3n, se utiliza el probador mec\u00e1nico Nanovea para evaluar la adhesi\u00f3n de seis muestras recubiertas.<br \/>\nutilizando la muestra m\u00faltiple <a title=\"prueba de resistencia al rayado\" href=\"https:\/\/nanovea.com\/micro-scratch-tester\" target=\"_blank\">prueba de resistencia al rayado<\/a>. Nos gustar\u00eda mostrar la capacidad de Nanovea Mechanical.<br \/>\nProbador para realizar pruebas de rayado automatizadas en m\u00faltiples muestras con alta eficiencia y<br \/>\nreproducibilidad.<\/p>\n<p><a title=\"prueba de rayado m\u00faltiple\" href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/multi-sample-scratch-test.pdf\" target=\"_blank\">Prueba de rayado automatizada de m\u00faltiples muestras<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In this application, the Nanovea Mechanical Tester is used to evaluate the adhesion of six coated samples using the multi sample scratch test. We would like to showcase the capacity of Nanovea Mechanical Tester in performing automated scratch tests on multiple samples with high efficiency and reproducibility. Automated Multi Sample Scratch Testing<\/p>","protected":false},"author":1,"featured_media":859,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[53],"class_list":["post-858","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-multi-scratch-testing"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts\/858","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/comments?post=858"}],"version-history":[{"count":4,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts\/858\/revisions"}],"predecessor-version":[{"id":11381,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts\/858\/revisions\/11381"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/media\/859"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/media?parent=858"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/categories?post=858"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/tags?post=858"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}