{"id":3389,"date":"2018-06-04T17:32:59","date_gmt":"2018-06-04T17:32:59","guid":{"rendered":"https:\/\/nanovea.com\/?p=3389"},"modified":"2018-06-04T17:32:59","modified_gmt":"2018-06-04T17:32:59","slug":"cuero-friccion-textil-tribologia","status":"publish","type":"post","link":"https:\/\/nanovea.com\/es\/leather-friction-textile-tribology\/","title":{"rendered":"Coeficiente de fricci\u00f3n del cuero utilizando un trib\u00f3metro"},"content":{"rendered":"<p>La fricci\u00f3n del cuero (COF) es muy importante para este material, ya que puede utilizarse para caracterizar propiedades como la resistencia al deslizamiento, el acabado y la degradaci\u00f3n del material. En el caso del cuero utilizado en el calzado, la resistencia al deslizamiento debe ser suficientemente alta. La resistencia al deslizamiento puede caracterizarse observando el COF est\u00e1tico y el COF din\u00e1mico con un <a href=\"https:\/\/nanovea.com\/tribometers\/\">Trib\u00f3metro<\/a>. El COF tambi\u00e9n determina la cantidad de fricci\u00f3n que se produce al frotar dos superficies entre s\u00ed. Esto puede utilizarse para determinar la calidad est\u00e9tica y la durabilidad del acabado del cuero cuando se aplica a prendas de vestir, herramientas y tapicer\u00edas.<\/p>\n<p><a href=\"http:\/\/nanovea.com\/App-Notes\/leather-friction.pdf\">Coeficiente de fricci\u00f3n del cuero utilizando un trib\u00f3metro<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>Leather friction (COF) is quite important for leather since it can be used to characterize properties such as slip resistance, finish and material degradation. For leather used in footwear, the slip resistance must be sufficiently high. Slip resistance can be characterized by observing the static COF and dynamic COF with a Tribometer. COF also determines [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":3385,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[314],"class_list":["post-3389","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-leather-friction"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts\/3389","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/comments?post=3389"}],"version-history":[{"count":1,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts\/3389\/revisions"}],"predecessor-version":[{"id":3390,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts\/3389\/revisions\/3390"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/media\/3385"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/media?parent=3389"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/categories?post=3389"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/tags?post=3389"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}