{"id":2646,"date":"2016-11-29T21:21:46","date_gmt":"2016-11-29T21:21:46","guid":{"rendered":"http:\/\/nanovea.com\/?p=2646"},"modified":"2016-11-29T21:22:08","modified_gmt":"2016-11-29T21:22:08","slug":"tribologia-inspeccion","status":"publish","type":"post","link":"https:\/\/nanovea.com\/es\/tribology-inspection\/","title":{"rendered":"Inspecci\u00f3n tribol\u00f3gica de recubrimientos de nitruro de titanio mediante trib\u00f3metro"},"content":{"rendered":"<p>El desgaste de las herramientas en servicio provoca la p\u00e9rdida de dimensiones y funcionalidad de las mismas. Esto influye significativamente en la vida \u00fatil de la herramienta, as\u00ed como en la integridad de la superficie y la precisi\u00f3n dimensional de los productos acabados. Las propiedades tribomec\u00e1nicas de los recubrimientos cer\u00e1micos protectores pueden mejorar sustancialmente el rendimiento y la vida \u00fatil de las m\u00e1quinas herramienta. Una inspecci\u00f3n tribol\u00f3gica fiable y precisa de dichos recubrimientos protectores resulta fundamental para garantizar el rendimiento de calidad de las herramientas.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/App-Notes\/tribology-inspection.pdf\">Inspecci\u00f3n de recubrimientos de nitruro de titanio mediante trib\u00f3metro<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>Wear of the tools in service creates loss of dimensions and functionality of the tools. It has significant influence on the tool life, as well as the surface integrity and dimension accuracy of the finished products. The tribo-mechanical properties of the protective ceramic coatings can substantially enhance the service performance and lifespan of the machine [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":2638,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7],"tags":[263],"class_list":["post-2646","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","tag-tribology-inspection"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts\/2646","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/comments?post=2646"}],"version-history":[{"count":1,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts\/2646\/revisions"}],"predecessor-version":[{"id":2647,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/posts\/2646\/revisions\/2647"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/media\/2638"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/media?parent=2646"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/categories?post=2646"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/es\/wp-json\/wp\/v2\/tags?post=2646"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}