{"id":949,"date":"2014-04-07T13:32:21","date_gmt":"2014-04-07T13:32:21","guid":{"rendered":"http:\/\/nanovea.com\/?p=949"},"modified":"2023-11-13T23:41:47","modified_gmt":"2023-11-13T23:41:47","slug":"nano-mikro-bio-tribologie-von-endokardialen-leitern-im-schank-losung","status":"publish","type":"post","link":"https:\/\/nanovea.com\/de\/nano-micro-bio-tribology-of-endocardial-leads-in-hanks-solution\/","title":{"rendered":"Biotribologie endokardialer Ableitungen in Hanks' L\u00f6sung"},"content":{"rendered":"<p>In dieser Studie haben wir das Nano-Reibungs- und Verschlei\u00dfverhalten von endokardialen Schrittmacherleitungen aus verschiedenen Materialien in Hanks Solution mit dem Nanovea simuliert und verglichen <a href=\"https:\/\/nanovea.com\/mechanical-testers\/\">Mechanisch<\/a> und <a title=\"Tribometer\" href=\"https:\/\/nanovea\/tribometers\" target=\"_blank\" rel=\"noopener noreferrer\">Tribometer<\/a>.<\/p>\n<p><a href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/Bio-Tribology.pdf\">Nano-Mikro-Biotribologie endokardialer Elektroden in Hanks' L\u00f6sung<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In dieser Studie simulierten und verglichen wir das Nanoreibungs- und Verschlei\u00dfverhalten von endokardialen Schrittmacherelektroden aus verschiedenen Materialien in Hanks'scher L\u00f6sung unter Verwendung des Nanovea Mechanical und Tribometers. Nano-Mikro-Biotribologie von endokardialen Elektroden in Hanks'scher L\u00f6sung<\/p>","protected":false},"author":1,"featured_media":951,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7,348],"tags":[132],"class_list":["post-949","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","category-friction-testing-coefficient-of-friction","tag-bio-tribology"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/949","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/comments?post=949"}],"version-history":[{"count":5,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/949\/revisions"}],"predecessor-version":[{"id":23505,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/949\/revisions\/23505"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/media\/951"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/media?parent=949"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/categories?post=949"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/tags?post=949"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}