{"id":942,"date":"2014-05-05T13:23:39","date_gmt":"2014-05-05T13:23:39","guid":{"rendered":"http:\/\/nanovea.com\/?p=942"},"modified":"2019-07-31T14:46:54","modified_gmt":"2019-07-31T14:46:54","slug":"oberflachenanalyse-von-kohlenstoff-zeolith-katalysatoren-mit-3d-profilometrie","status":"publish","type":"post","link":"https:\/\/nanovea.com\/de\/surface-analysis-of-carbon-zeolite-catalysts-using-3d-profilometry\/","title":{"rendered":"Oberfl\u00e4chenanalyse von Kohlenstoff- und Zeolith-Katalysatoren mit 3D-Profilometrie"},"content":{"rendered":"<p>In dieser Anwendung wird das Nanovea ST400 <a title=\"profilometer\" href=\"https:\/\/https:\/\/nanovea.com\/profilometers\" target=\"_blank\" rel=\"noopener noreferrer\">Profilometer<\/a> wird zur Messung der Oberfl\u00e4che von Kohlenstoff- und Zeolithkatalysatoren verwendet. Die gemessene Fl\u00e4che wurde nach dem Zufallsprinzip ausgew\u00e4hlt und als gro\u00df genug angenommen, um Annahmen \u00fcber eine viel gr\u00f6\u00dfere Oberfl\u00e4che treffen zu k\u00f6nnen. Die Oberfl\u00e4chenrauhigkeit und die entwickelte Fl\u00e4che werden zur Charakterisierung der verf\u00fcgbaren Oberfl\u00e4che verwendet.<\/p>\n<p><a title=\"Oberfl\u00e4chenanalyse\" href=\"https:\/\/nanovea.com\/wp-content\/themes\/wp-nanovea\/Application%20Notes\/surface-analysis-carbon.pdf\" target=\"_blank\" rel=\"noopener noreferrer\">Oberfl\u00e4chenanalyse von Kohlenstoff- und Zeolith-Katalysatoren mit 3D-Profilometrie<\/a><\/p>","protected":false},"excerpt":{"rendered":"<p>In this application the Nanovea ST400 Profilometer is used to measure the surface of carbon and zeolite catalysts. The area measured was selected at random, and assumed large enough in that it could be extrapolated to make assumptions about a much larger surface. Surface roughness and developed area will be used to characterize the available [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":943,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7,355],"tags":[80],"class_list":["post-942","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","category-profilometry-volume-area","tag-surface-analysis"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/942","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/comments?post=942"}],"version-history":[{"count":5,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/942\/revisions"}],"predecessor-version":[{"id":6632,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/942\/revisions\/6632"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/media\/943"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/media?parent=942"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/categories?post=942"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/tags?post=942"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}