{"id":23217,"date":"2023-09-13T17:07:17","date_gmt":"2023-09-13T17:07:17","guid":{"rendered":"https:\/\/nanovea.com\/?p=23217"},"modified":"2025-05-22T19:02:58","modified_gmt":"2025-05-22T19:02:58","slug":"prufung-der-abrasivitat-von-gestein","status":"publish","type":"post","link":"https:\/\/nanovea.com\/de\/rock-abrasivity-testing\/","title":{"rendered":"Gesteinsabriebpr\u00fcfung mit NANOVEA Tribometer"},"content":{"rendered":"<div data-elementor-type=\"wp-post\" data-elementor-id=\"23217\" class=\"elementor elementor-23217\" data-elementor-post-type=\"post\">\n\t\t\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-8e47bb1 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"8e47bb1\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-b2a27af\" data-id=\"b2a27af\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-5ccc488 elementor-widget elementor-widget-text-editor\" data-id=\"5ccc488\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<h1 style=\"text-align: center; font-style: italic; font-weight: bold;\"><span style=\"font-size: 80px; color: #1b96cf; display: block;\">ROCK-TRIBOLOGIE:<\/span><span style=\"font-size: 32px; color: #000;\">ROCK-ABRASIVIT\u00c4TSPR\u00dcFUNG MIT DEM NANOVEA-TRIBOMETER<\/span><\/h1>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-f972c31 elementor-widget elementor-widget-image\" data-id=\"f972c31\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2023\/09\/rock-tribology-NANOVEA.jpg\" title=\"\" alt=\"ROCK TRIBOLOGY: Pr\u00fcfung der Abrasivit\u00e4t von Gestein mit dem NANOVEA-Tribometer\" loading=\"lazy\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-1ff7eff elementor-widget elementor-widget-heading\" data-id=\"1ff7eff\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Vorbereitet von<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-7373652 elementor-widget elementor-widget-heading\" data-id=\"7373652\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">DUANJIE LI, PhD<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-390b389 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"390b389\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-273aa4d\" data-id=\"273aa4d\" data-element_type=\"column\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-88d057b elementor-widget elementor-widget-heading\" data-id=\"88d057b\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">EINF\u00dcHRUNG<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-0476635 elementor-widget elementor-widget-text-editor\" data-id=\"0476635\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\tGesteine bestehen aus Mineralk\u00f6rnern. Die Art und H\u00e4ufigkeit dieser Mineralien sowie die chemische Bindungsst\u00e4rke zwischen den Mineralk\u00f6rnern bestimmen die mechanischen und tribologischen Eigenschaften der Gesteine. Abh\u00e4ngig von den geologischen Gesteinszyklen k\u00f6nnen Gesteine Transformationen durchlaufen und werden typischerweise in drei Haupttypen eingeteilt: magmatisch, sediment\u00e4r und metamorph. Diese Gesteine weisen unterschiedliche mineralische und chemische Zusammensetzungen, Permeabilit\u00e4ten und Partikelgr\u00f6\u00dfen auf, und diese Eigenschaften tragen zu ihrer unterschiedlichen Verschlei\u00dffestigkeit bei. Die Gesteinstribologie untersucht das Verschlei\u00df- und Reibungsverhalten von Gesteinen unter verschiedenen geologischen und Umweltbedingungen.\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-b4c4ec7 elementor-widget elementor-widget-heading\" data-id=\"b4c4ec7\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">BEDEUTUNG DER PR\u00dcFUNG VON STEINABRASIVMITTELN<\/h3>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-3b72871 elementor-widget elementor-widget-text-editor\" data-id=\"3b72871\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>W\u00e4hrend des Bohrvorgangs von Bohrl\u00f6chern treten verschiedene Arten der Abnutzung des Gesteins, einschlie\u00dflich Abrieb und Reibung, auf, was zu erheblichen direkten Verlusten und Folgeverlusten f\u00fchrt, die auf die Reparatur und den Austausch von Bohrern und Schneidwerkzeugen zur\u00fcckzuf\u00fchren sind. Daher ist die Untersuchung der Bohrbarkeit, Bohrbarkeit, Schneidbarkeit und Abrasivit\u00e4t von Gesteinen in der \u00d6l-, Gas- und Bergbauindustrie von entscheidender Bedeutung. Die Gesteinstribologieforschung spielt eine entscheidende Rolle bei der Auswahl der effizientesten und kosteng\u00fcnstigsten Bohrstrategien, steigert dadurch die Gesamteffizienz und tr\u00e4gt zur Einsparung von Materialien, Energie und Umwelt bei. Dar\u00fcber hinaus ist die Minimierung der Oberfl\u00e4chenreibung \u00e4u\u00dferst vorteilhaft, da sie die Wechselwirkung zwischen Bohrmei\u00dfel und Gestein verringert, was zu einem geringeren Werkzeugverschlei\u00df und einer verbesserten Bohr-\/Schneideffizienz f\u00fchrt.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-6202d16 elementor-reverse-mobile elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"6202d16\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-6dae397\" data-id=\"6dae397\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-d6dd9bb elementor-widget elementor-widget-heading\" data-id=\"d6dd9bb\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">MESSZIEL<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-b5057e1 elementor-widget elementor-widget-text-editor\" data-id=\"b5057e1\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>In dieser Studie haben wir die tribologischen Eigenschaften zweier Gesteinsarten simuliert und verglichen, um die Leistungsf\u00e4higkeit des <a href=\"https:\/\/nanovea.com\/instruments\/t50\/\">NANOVEA T50 Tribometer<\/a> bei der kontrollierten und \u00fcberwachten Messung des Reibungskoeffizienten und der Verschlei\u00dfrate von Gesteinen.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<section class=\"elementor-section elementor-inner-section elementor-element elementor-element-cebd155 elementor-reverse-mobile elementor-section-full_width elementor-reverse-tablet elementor-section-height-default elementor-section-height-default\" data-id=\"cebd155\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-no\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-50 elementor-inner-column elementor-element elementor-element-7c681e0\" data-id=\"7c681e0\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-90b5504 elementor-widget elementor-widget-text-editor\" data-id=\"90b5504\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p style=\"text-align: center; font-size: 20pt; color: black;\">NANOVEA <span style=\"font-size: 20pt; color: #1b96cf;\">T50 Kompakt<\/span><br>Tribometer mit freiem Gewicht<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-b34cd8b e-grid e-con-full e-con e-child\" data-id=\"b34cd8b\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-499294e elementor-align-center homepage-button-brochure elementor-widget elementor-widget-button\" data-id=\"499294e\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"https:\/\/nanovea.com\/t50-tribometer-brochure-form\/\" id=\"homepage-button-brochure\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">BROSCH\u00dcRE HERUNTERLADEN<\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-0e8a245 elementor-align-center homepage-button-quote elementor-widget elementor-widget-button\" data-id=\"0e8a245\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"https:\/\/nanovea.com\/contact-sales-form\/\" id=\"homepage-button-quote\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">ANGEBOT EINHOLEN<\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t<div class=\"elementor-column elementor-col-50 elementor-inner-column elementor-element elementor-element-b00d07e\" data-id=\"b00d07e\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-6de9b1a elementor-widget elementor-widget-image\" data-id=\"6de9b1a\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<a href=\"https:\/\/nanovea.com\/instruments\/t50\/\">\n\t\t\t\t\t\t\t<img fetchpriority=\"high\" decoding=\"async\" width=\"434\" height=\"432\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2023\/06\/NANOVEA-T50-Tribometer-for-Wear-Test.jpg\" class=\"elementor-animation-grow attachment-medium_large size-medium_large wp-image-22861\" alt=\"NANOVEA TRIBOMETER: Pr\u00fcfung der Abrasivit\u00e4t von Kalkstein und Marmor\" \/>\t\t\t\t\t\t\t\t<\/a>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t<div class=\"elementor-element elementor-element-7c281f4 e-flex e-con-boxed e-con e-parent\" data-id=\"7c281f4\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-f11929c elementor-widget elementor-widget-heading\" data-id=\"f11929c\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">DIE MUSTER<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-c432949 elementor-widget elementor-widget-image\" data-id=\"c432949\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2023\/09\/marble-and-limestone-wear-and-friction.jpg\" title=\"\" alt=\"Verschlei\u00df- und Reibungspr\u00fcfung von Marmor und Kalkstein \u2013 Gesteinstribologie\" loading=\"lazy\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-09a60f5 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"09a60f5\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-narrow\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-e692062\" data-id=\"e692062\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-165267f elementor-widget elementor-widget-heading\" data-id=\"165267f\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">TESTVORGANG<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-ed3663d elementor-widget elementor-widget-text-editor\" data-id=\"ed3663d\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Der Reibungskoeffizient, COF und die Verschlei\u00dffestigkeit von zwei Gesteinsproben wurden mit dem NANOVEA T50 Tribometer unter Verwendung des Pin-on-Disc-Verschlei\u00dfmoduls bewertet. Als Gegenmaterial wurde eine Al2O3-Kugel (6 mm Durchmesser) verwendet. Nach den Tests wurde die Verschlei\u00dfspur mit dem NANOVEA Non-Contact Profilometer untersucht. Nachfolgend sind die Testparameter zusammengefasst.<\/p><p>Die Verschlei\u00dfrate K wurde mithilfe der Formel K=V\/(F\u00d7s)=A\/(F\u00d7n) bewertet, wobei V das verschlissene Volumen, F die normale Belastung, s die Gleitstrecke und A ist die Querschnittsfl\u00e4che der Verschlei\u00dfspur und n ist die Anzahl der Umdrehungen. Oberfl\u00e4chenrauheit und Verschlei\u00dfspurprofile wurden mit dem NANOVEA Optical Profilometer bewertet und die Verschlei\u00dfspurmorphologie wurde mit einem optischen Mikroskop untersucht.<\/p><p>Bitte beachten Sie, dass in dieser Studie als Beispiel die Al2O3-Kugel als Gegenmaterial verwendet wurde. Jedes feste Material mit unterschiedlichen Formen kann mit einer ma\u00dfgeschneiderten Vorrichtung aufgetragen werden, um die tats\u00e4chliche Anwendungssituation zu simulieren.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-7be119b elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"7be119b\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-no\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-4e700fa\" data-id=\"4e700fa\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-48cce8f elementor-widget elementor-widget-heading\" data-id=\"48cce8f\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">PR\u00dcFPARAMETER<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-44e1928 elementor-widget elementor-widget-text-editor\" data-id=\"44e1928\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<table style=\"border-collapse: collapse; width: 100%;\">\n<tbody>\n<tr>\n<td style=\"width: 50%; text-align: left;\"><em><strong style=\"color: #1b96cf;\">PROBEN<\/strong><\/em><\/td>\n<td style=\"width: 52.497%; text-align: right;\"><em><strong>Kalkstein, Marmor<\/strong><\/em><\/td>\n<\/tr>\n<tr>\n<td style=\"width: 50%; text-align: left;\"><em><strong style=\"color: #1b96cf;\">VERSCHLEISSRINGRADIUS <\/strong><\/em><\/td>\n<td style=\"width: 52.497%; text-align: right;\"><em><strong>5 mm<\/strong><\/em><\/td>\n<\/tr>\n<tr>\n<td style=\"width: 50%; text-align: left;\"><em><strong style=\"color: #1b96cf;\">NORMALE KRAFT<\/strong><\/em><\/td>\n<td style=\"width: 52.497%; text-align: right;\"><em><strong>10 N<\/strong><\/em><\/td>\n<\/tr>\n<tr>\n<td style=\"width: 50%; text-align: left;\"><em><strong style=\"color: #1b96cf;\">TESTDAUER<\/strong><\/em><\/td>\n<td style=\"width: 52.497%; text-align: right;\"><em><strong>10 Minuten<\/strong><\/em><\/td>\n<\/tr>\n<tr>\n<td style=\"width: 50%; text-align: left;\"><em><strong style=\"color: #1b96cf;\">SPEED<\/strong><\/em><\/td>\n<td style=\"width: 52.497%; text-align: right;\"><em><strong>100 U\/min<\/strong><\/em><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-aef3573 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"aef3573\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-e4a16d3\" data-id=\"e4a16d3\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-3707fef elementor-widget elementor-widget-heading\" data-id=\"3707fef\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">ERGEBNISSE &amp; DISKUSSION<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-64378be elementor-widget elementor-widget-text-editor\" data-id=\"64378be\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>Die H\u00e4rte (H) und der Elastizit\u00e4tsmodul (E) der Kalkstein- und Marmorproben werden in ABBILDUNG 1 unter Verwendung des Micro Indentation-Moduls des NANOVEA Mechanical Tester verglichen. Die Kalksteinprobe wies mit 0,53 bzw. 25,9 GPa niedrigere H- und E-Werte auf, im Gegensatz zu Marmor, der Werte von 1,07 f\u00fcr H und 49,6 GPa f\u00fcr E aufwies. Die relativ h\u00f6here Variabilit\u00e4t der H- und E-Werte, die in beobachtet wurde Die Kalksteinprobe ist auf ihre gr\u00f6\u00dfere Oberfl\u00e4cheninhomogenit\u00e4t zur\u00fcckzuf\u00fchren, die auf ihre k\u00f6rnigen und por\u00f6sen Eigenschaften zur\u00fcckzuf\u00fchren ist.<\/p><p>Die Entwicklung des COF w\u00e4hrend der Verschlei\u00dftests der beiden Gesteinsproben ist in ABBILDUNG 2 dargestellt. Der Kalkstein erf\u00e4hrt zu Beginn des Verschlei\u00dftests zun\u00e4chst einen schnellen Anstieg des COF auf etwa 0,8 und beh\u00e4lt diesen Wert w\u00e4hrend der gesamten Testdauer bei. Diese abrupte COF-\u00c4nderung kann auf das Eindringen der Al2O3-Kugel in die Gesteinsprobe zur\u00fcckgef\u00fchrt werden, was auf einen schnellen Verschlei\u00df- und Aufrauungsprozess an der Kontaktfl\u00e4che innerhalb der Verschlei\u00dfspur zur\u00fcckzuf\u00fchren ist. Im Gegensatz dazu zeigt die Marmorprobe nach etwa 5 Metern Gleitstrecke einen deutlichen Anstieg des COF auf h\u00f6here Werte, was auf ihre \u00fcberlegene Verschlei\u00dffestigkeit im Vergleich zum Kalkstein hinweist.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-4c483d4 elementor-widget elementor-widget-image\" data-id=\"4c483d4\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2023\/09\/rock-hardness-test-NANOVEA.jpg\" title=\"\" alt=\"Gesteinsh\u00e4rtepr\u00fcfung\" loading=\"lazy\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-8a573c9 elementor-widget elementor-widget-text-editor\" data-id=\"8a573c9\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p style=\"text-align: center;\"><span class=\"fontstyle0\" style=\"color: #1b96cf;\">ABBILDUNG 1:<\/span><span class=\"fontstyle0\" style=\"color: #000000;\">\u00a0Vergleich der H\u00e4rte und des Elastizit\u00e4tsmoduls zwischen Kalkstein- und Marmorproben.<\/span><\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-ad658da elementor-widget elementor-widget-image\" data-id=\"ad658da\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2023\/09\/Coefficient-of-Friction-Marble-and-Limestone.jpg\" title=\"\" alt=\"Entwicklung des Reibungskoeffizienten (COF) in Kalkstein- und Marmorproben w\u00e4hrend Verschlei\u00dftests\" loading=\"lazy\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-1755171 elementor-widget elementor-widget-text-editor\" data-id=\"1755171\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p style=\"text-align: center;\"><span class=\"fontstyle0\" style=\"color: #1b96cf;\">ABBILDUNG 2:<\/span><span class=\"fontstyle0\" style=\"color: #000000;\"> Entwicklung des Reibungskoeffizienten (COF) in Kalkstein- und Marmorproben w\u00e4hrend Verschlei\u00dftests.<\/span><\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-242dcd0 elementor-widget elementor-widget-text-editor\" data-id=\"242dcd0\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\tABBILDUNG 3 vergleicht die Querschnittsprofile der Kalkstein- und Marmorproben nach den Verschlei\u00dftests und Tabelle 1 fasst die Ergebnisse der Verschlei\u00dfspuranalyse zusammen. ABBILDUNG 4 zeigt die Verschlei\u00dfspuren der Proben unter dem Lichtmikroskop. Die Bewertung der Verschlei\u00dfspur stimmt mit der Beobachtung der COF-Entwicklung \u00fcberein: Die Marmorprobe, die \u00fcber einen l\u00e4ngeren Zeitraum einen niedrigen COF beibeh\u00e4lt, weist eine geringere Verschlei\u00dfrate von 0,0046 mm\u00b3\/N m auf, verglichen mit 0,0353 mm\u00b3\/N m beim Kalkstein. Die \u00fcberlegenen mechanischen Eigenschaften von Marmor tragen zu einer besseren Verschlei\u00dffestigkeit als Kalkstein bei.\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-1a5b954 elementor-widget elementor-widget-image\" data-id=\"1a5b954\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2023\/09\/rock-wear-tester.jpg\" title=\"\" alt=\"ROCK-ABRASIVIT\u00c4TSPR\u00dcFUNG MIT DEM NANOVEA-TRIBOMETER\" loading=\"lazy\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-675b30d elementor-widget elementor-widget-text-editor\" data-id=\"675b30d\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p style=\"text-align: center;\"><span class=\"fontstyle0\" style=\"color: #1b96cf;\">ABBILDUNG 3:<\/span><span class=\"fontstyle0\" style=\"color: #000000;\">\u00a0Querschnittsprofile der Verschlei\u00dfspuren.<\/span><\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-3cd0cdd elementor-widget elementor-widget-image\" data-id=\"3cd0cdd\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" width=\"1077\" height=\"200\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2023\/09\/rock-tribology-testing-using-NANOVEA-Tribometer.jpg\" class=\"attachment-full size-full wp-image-24670\" alt=\"\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-b269c04 elementor-widget elementor-widget-text-editor\" data-id=\"b269c04\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p style=\"text-align: center;\"><span class=\"fontstyle0\" style=\"color: #1b96cf;\">TABELLE 1:<\/span><span class=\"fontstyle0\" style=\"color: #000000;\">\u00a0Ergebniszusammenfassung der Verschlei\u00dfspuranalyse.<\/span><\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-a1688e7 elementor-widget elementor-widget-image\" data-id=\"a1688e7\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" width=\"876\" height=\"419\" src=\"https:\/\/nanovea.com\/wp-content\/uploads\/2023\/09\/limestone-and-marble-tribometer-testing.jpg\" class=\"attachment-large size-large wp-image-24671\" alt=\"\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-af84c18 elementor-widget elementor-widget-text-editor\" data-id=\"af84c18\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p style=\"text-align: center;\"><span class=\"fontstyle0\" style=\"color: #1b96cf;\">ABBILDUNG 4:<\/span><span class=\"fontstyle0\" style=\"color: #000000;\">\u00a0Abnutzungsspuren unter dem Lichtmikroskop.<\/span><\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-6167248 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"6167248\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-19529d4\" data-id=\"19529d4\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-41f8947 elementor-widget elementor-widget-heading\" data-id=\"41f8947\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">SCHLUSSFOLGERUNG<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<section class=\"elementor-section elementor-inner-section elementor-element elementor-element-066782b elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"066782b\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-inner-column elementor-element elementor-element-74941d5\" data-id=\"74941d5\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-a934044 elementor-widget elementor-widget-text-editor\" data-id=\"a934044\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<p>In dieser Studie haben wir die F\u00e4higkeit des NANOVEA Tribometers demonstriert, den Reibungskoeffizienten und die Verschlei\u00dffestigkeit von zwei Gesteinsproben, n\u00e4mlich Marmor und Kalkstein, auf kontrollierte und \u00fcberwachte Weise zu bewerten. Die hervorragenden mechanischen Eigenschaften von Marmor tragen zu seiner au\u00dfergew\u00f6hnlichen Verschlei\u00dffestigkeit bei. Diese Eigenschaft macht das Bohren oder Schneiden in der \u00d6l- und Gasindustrie zu einer Herausforderung. Umgekehrt verl\u00e4ngert es seine Lebensdauer deutlich, wenn es als hochwertiger Baustoff, beispielsweise als Bodenfliese, verwendet wird.<\/p><p>NANOVEA-Tribometer bieten pr\u00e4zise und wiederholbare Verschlei\u00df- und Reibungstestfunktionen und entsprechen den ISO- und ASTM-Standards sowohl im Rotations- als auch im Linearmodus. Dar\u00fcber hinaus bietet es optionale Module f\u00fcr Hochtemperaturverschlei\u00df, Schmierung und Tribokorrosion, die alle nahtlos in ein System integriert sind. Das un\u00fcbertroffene Sortiment von NANOVEA ist eine ideale L\u00f6sung zur Bestimmung des gesamten Spektrums tribologischer Eigenschaften d\u00fcnner oder dicker, weicher oder harter Beschichtungen, Filme, Substrate und Gesteinstribologie.<\/p>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-5b31b52 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"5b31b52\" data-element_type=\"section\">\n\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-f518474\" data-id=\"f518474\" data-element_type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-9f8cde6 elementor-widget elementor-widget-heading\" data-id=\"9f8cde6\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">Haben Sie eine \u00e4hnliche Anwendung?<\/h2>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-377d6ab elementor-align-justify open-chat elementor-widget elementor-widget-button\" data-id=\"377d6ab\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-size-sm\" role=\"button\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">JETZT MIT EINEM EXPERTEN DISKUTIEREN<\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-08a11b4 elementor-align-justify button-quote elementor-widget elementor-widget-button\" data-id=\"08a11b4\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"https:\/\/nanovea.com\/contact-sales-form\/\" id=\"button-quote-bottom\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">PREISE UND DETAILS SCHNELL ERHALTEN<\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<\/div>","protected":false},"excerpt":{"rendered":"<p>ROCK TRIBOLOGY:ROCK ABRASIVITY TESTING USING NANOVEA TRIBOMETER Prepared by DUANJIE LI, PhD INTRODUCTION Rocks are composed of grains of minerals. The type and abundance of these minerals, as well as the chemical bonding strength between the mineral grains, determine the mechanical and tribological properties of the rocks. Depending on the geological rock cycles, rocks can [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":24150,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_exactmetrics_skip_tracking":false,"_exactmetrics_sitenote_active":false,"_exactmetrics_sitenote_note":"","_exactmetrics_sitenote_category":0,"footnotes":""},"categories":[7,349,373,336],"tags":[],"class_list":["post-23217","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-application-notes","category-laboratory-testing","category-rotational-tribology","category-tribology-testing"],"_links":{"self":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/23217","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/comments?post=23217"}],"version-history":[{"count":38,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/23217\/revisions"}],"predecessor-version":[{"id":24679,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/posts\/23217\/revisions\/24679"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/media\/24150"}],"wp:attachment":[{"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/media?parent=23217"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/categories?post=23217"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/nanovea.com\/de\/wp-json\/wp\/v2\/tags?post=23217"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}